J557SLA、J557SLB Low Hydrogen Welding Rod AWS E8015-G Low Alloy Stick Electrodes for Arc Welding

Tlhaloso e Khutšoanyane:

Ena ke sodium e tlase ea haedrojene e koahetsoeng ka electrode e khethehileng bakeng sa tšepe ea aluminiized.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

Electrode e tlase ea Alloy Steel Welding

J557SLA, J557SLB                                        

GB/T E5515-G

AWS E8015-G

Tlhaloso: Ena ke sodium e tlase ea hydrogen e koahetsoeng ka electrode e khethehileng bakeng sa tšepe ea aluminiized.Sebelisa DCEP (electrode e nepahetseng hona joale), 'me e ka chesetsoa maemong ohle ka ts'ebetso e khuts'oane ea arc.J557SLA e ka ts'oaroa ka kotloloho ntle le ho tlosa lesela le nang le aluminized holim'a groove pele ho welding.Empa J557SLB e lokela ho tlosa lera la aluminiized holim'a groove pele ho tjheseletsa.

Tšebeliso: E sebelisetsoa ho cheseletsa mohaho oa tšepe o entsoeng ka aluminiized tlas'a corrosion medium ea hydrogen sulfide, sulfur, ammonia, ammonium bicarbonate le hydrogen nitrogen e nang le mocheso o sebetsang o ka tlase ho 540 ° C.Joalo ka liphaephe tsa boiler, lisebelisoa tsa ho hloekisa peterole, lisebelisoa tsa manyolo le liphaephe tsa mouoane, jj.

 Sebopeho sa lik'hemik'hale tsa tšepe ea weld(%):

C

Mn

Si

Cr

Mo

Al

S

P

≤0.12

0,50 ~ 0,90

≤0.50

≈0.80

≥0.20

≤0.055

≤0.035

≤0.035

 Mechine ea tšepe ea weld:

Ntho ea teko

Matla a tšepe

Mpa

Ho hlahisa matla

Mpa

Elongation

%

Boleng ba tšusumetso (J)

Tloaelehileng Temp.

Guaranteed

≥540

≥440

≥17

≥49

 

Likahare tsa hydrogen tsa tšepe e kentsoeng: ≤6.0mL/100g (mokhoa oa glycerin)

 

Tlhahlobo ea X-ray: Ke ea sehlopheng

 

Nako e khothalelitsoeng:

(mm)

Bophara ba molamu

2.5

3.2

4.0

5.0

(A)

Welding Current

Lilemo tse 50-80

80 ~ 110

130 ~ 170

160 ~ 200

 

Tlhokomeliso:

1. Electrode e tlameha ho behoa bakeng sa hora e le 1 ho pota 350 ℃ pele ho ts'ebetso ea welding;

2. Ho bohlokoa ho hloekisa mafome, sekala sa oli, metsi le litšila holim'a likarolo tsa ho tjheseletsa pele ho tjheseletsa.


  • E fetileng:
  • E 'ngoe: