Nickel Alloy Welding Wire ERNiCrMo-3 Mig Welding Wire

Tlhaloso e Khutšoanyane:

ERNiCrMo-3 ke terata e phahameng ea nickel alloy e etselitsoeng ho cheselletsa le ho roala li-alloys tse thehiloeng ho nickel joalo ka 625 kapa lisebelisoa tse tšoanang.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

Nickel AlloyWelding WireERNiCrMo-3

 

Litekanyetso

EN ISO 18274 - Ni 6625 - NiCr22Mo9Nb

AWS A5.14 – ER NiCrMo-3

 

Likarolo le Lisebelisoa

Phahamengnikeleterata ea motsoako e etselitsoeng ho cheselletsa le ho roalanikeleli-alloys tse thehiloeng joalo ka 625 kapa lisebelisoa tse tšoanang.

E tiileng e huleloa ka mokhoa o ikhethileng oa ho fumana litšepe tse hloekileng le tsa boleng bo holimo tse nang le seam e khanyang le ductility e ntle haholo.

Tšepe ea weld e na le thepa e ntle haholo ea mochini mocheso o phahameng le o tlase.

Ho hanyetsa hantle ho pitting le khatello ea maikutlo.

Thempereichara ea ho sebetsa e khothalelitsoeng ho tloha ho cryogenic ho isa ho 540°C.

Precision layer leqeba bakeng sa litšobotsi tse phahameng tsa ho fepa ka terata.

Ka tloaelo e sebelisoa indastering ea tšebetso ea lik'hemik'hale, boenjineri ba leoatleng, likarolo tsa nyutlelie, sepakapaka le ka har'a lisebelisoa tsa taolo ea tšilafalo jj.

 

Lisebelisoa tse Tloaelehileng tsa Base

Inconel 601, Incoloy 800, Alloy 625, Alloy 825, Alloy 926* * Lethathamo la litšoantšo, eseng le felletseng

 

Sebopeho sa Lik'hemik'hale %

C%

Mn%

Fe%

P%

S%

Si%

Cu%

max

max

max

max

max

max

max

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ni%

Co%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

max

max

max

20.00

3.15

8.00

Min

1.0

0.40

0.40

23.00

4.15

10.00

 

Thepa ea Mechini

Matla a tšepe

≥760 MPa

Kotulo Matla

≥415 MPa

Elongation

≥35%

Matla a Tšusumetso

≥100 J

Thepa ea mechine e hakanngoa 'me e ka fapana ho latela mocheso, khase e sireletsang, li-parameter tsa welding le lintlha tse ling.

Likhase Tsa Tšireletso

TS EN ISO 14175 - I1, I3

Maemo a Welding

EN ISO 6947 - PA, PB, PC, PD, PE, PF

Lintlha tsa ho paka

Diameter

Boima ba 'mele

Spool

Pallet Qty

1.00 limilimithara

1.20 limilimithara

15 Kg

15 Kg

BS300

BS300

72

72