AWS E10015-G (J707Ni) Ho Wellisa Tšepe e Tlase e nang le Alloy e Tlase

Tlhaloso e Khutšoanyane:

J707Ni (AWS E10015-G) ke electrode ea tšepe e matla e nang le motsoako o tlase e nang le sekoahelo sa sodium e fokolang ea haeterojene.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Tlaase AlloyHo tjheseletsa ka TšepeElektrode

J707Ni                               

GB/T E7015-G

AWS E10015-G

 

Tlhaloso: J707Ni ke electrode ea tšepe e matla e nang le motsoako o tlase e nang le sodium e tlase ea haedrojene. Sebelisa DCEP (electrode ea hona joale e tobileng e ntle) 'me e ka kopanngoa libakeng tsohle. Tšepe e kentsoeng e na le thepa e ntle ea mechini. Ha e bapisoa le electrode ea J707, tšobotsi e ka sehloohong ea J707Ni ke hore ho tiea ha mocheso o tlase le ho hanyetsa mapetso li ntlafalitsoe haholo.

Tšebeliso: E sebelisoa bakeng sa ho tjheseletsa meaho ea tšepe e nang le molo o tlase oa matla a lekanang, joalo ka 14MnMoVB, WEL-TEN70 le Japanese HW56 le meaho e meng ea tšepe e nang le molo o tlase oa matla a phahameng.

 

Sebopeho sa lik'hemik'hale sa tšepe e welded (%):

C

Si

Mn

Ni

Mo

Cr

S

P

≤0.10

≤0.60

≥1.00

1.80 ~ 2.20

0.40 ~ 0.60

≤0.20

≤0.030

≤0.030

 

Litšobotsi tsa mechini tsa tšepe e welded:

 

Ntho ea teko

 

Matla a tšepe

Mpa

 

Matla a tlhahiso

Mpa

 

Ho lelefatsa

%

 

Boleng ba tšusumetso (J)

-40℃

-50℃

 

E tiiselitsoe

≥690

≥590

≥15

—

≥27

 

E lekiloe

760

630

23

140

—

 

 

Tekanyo ea haedrojene e hasaneng ea tšepe e bolokiloeng: ≤4.0mL/100g (mokhoa oa glycerin) 

Tlhahlobo ea X-ray ea I: Kereiti ea I

 

Khoeli e khothaletsoang:

(mm)

Bophara ba molamu

2.5

3.2

4.0

5.0

(A)

ho tjheseletsa hona joale

60 ~ 100

100 ~ 140

140 ~ 190

190 ~ 250

 

 

Tsebiso:

1. Electrode e lokela ho besoa hora e le 'ngoe mochesong oa 350 ~380℃ pele ho ts'ebetso ea ho tjheseletsa;

2. Ho bohlokoa ho hlwekisa mafome, sekala sa oli, metsi le litšila likarolong tsa ho tjheseletsa pele ho tjheseletsa;

3. Sebelisa ts'ebetso e khutšoanyane ea arc ha u tjheseletsa. Tsela e moqotetsane ea ho tjheseletsa e loketse.

 