Stick Electrodes Low Alloy Steel Welding Rod AWS E8011-G le High Cellulose Potassium Coating

Tlhaloso e Khutšoanyane:

J555 (AWS E8011-G) ke electrode e theohileng tlase e nang le potassium e ngata ea cellulose.AC le DC merero e 'meli.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

J555

GB/T E5511-G

AWS E8011-G

Tlhaloso: J555 ke elektrode e theohileng e tlase e nang le potassium e ngata ea cellulose.AC le DC merero e 'meli.ha ho chesehela fatše, tšepe e qhibilihisitsoeng le slag li ke ke tsa phalla fatše.E na le matla a maholo a arc le ho kenella.tjheseletsa tlase ka thehoa ka mahlakoreng a mabeli 'me o na le phahameng tjheseletsa lebelo.

Kopo: E sebelisetsoa ho tjheseletsa liphaephe tsa tšepe tse tlaase.

Sebopeho sa lik'hemik'hale tsa tšepe ea weld(%):

C

Mn

Si

S

P

≤0.20

≥1.00

≤0.50

≤0.035

≤0.035

 

Mechine ea tšepe ea weld:

Ntho ea teko

Matla a tšepe

Mpa

Ho hlahisa matla

Mpa

Elongation

%

Boleng ba tšusumetso (J)

-30 ℃

Guaranteed

≥540

≥440

≥17

≥27

Tlhahlobo ea X-ray: Sehlopha sa II

 

Nako e khothalelitsoeng:

(mm)

Bophara ba molamu

2.5

3.2

4.0

5.0

(A)

Welding Current

Lilemo tse 45-75

80 ~ 120

130 ~ 160

170 ~ 190

 

Tlhokomeliso:

Electrode e tlameha ho behoa ka 70-90 ° C bakeng sa hora e le 'ngoe pele e sebelisoa.Mocheso ha oa lokela ho ba o phahameng haholo, ho seng joalo selulose ka ho roala e tla senyeha.

 

Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka 2000. Re se re ntse re etsa tlhahiso eaelectrode ea ho tjheseletsas, melamu ea ho cheselletsa, le lisebelisoa tsa ho cheselletsa ka lilemo tse fetang 20.

Lihlahisoa tsa rona tsa mantlha li kenyelletsa li-electrode tsa tšepe tse se nang tšepe, li-electrode tsa tšepe tsa carbon steel,li-electrode tse tlase tsa alloy welding, li-electrode tsa welding tse holim'a metsi, li-electrode tsa nickel & cobalt alloy welding, tšepe e bonolo & lithapo tse tlase tsa alloy, lithapo tsa tšepe tse sa hloekang, lithapo tse sirelelitsoeng ka khase, lithapo tsa aluminium, li-arc tse kentsoeng ka metsing.lithapo, lithapo tsa nickel & cobalt alloy welding, lithapo tsa tšepe tsa koporo, lithapo tsa welding tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tsa carbon gouging, le lisebelisoa tse ling tsa welding & consumables.

 


  • E fetileng:
  • E 'ngoe: