AWS E8018-C1 Mocheso o Tlaase oa Tšepe Welding Electrode W606Fe Low Hydrogen ARC Welding Rods

Tlhaloso e Khutšoanyane:

W606Fe (AWS E8018-C1) ke electrode ea tšepe e nang le mocheso o tlase o nang le phofo ea tšepe le ho roala ha hydrogen potassium.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

Mocheso o TlaseHo cheselletsa tšepeElectrode

W606Fe                                                     

GB/T E5518-C1

AWS A5.5 E8018-C1

Tlhaloso: W606Fe ke electrode ea tšepe e nang le mocheso o tlase o nang le phofo ea tšepe le ho roala ha hydrogen potassium.E ka sebelisoa bakeng sa tjheseletsa ea maemo ohle ka AC le DC.Tšepe e kentsoeng e na le matla a matla a tšusumetso ho -60°C. 

Kopo: E sebelisetsoa ho tjheseletsa tšepe ea mocheso o tlase joalo ka 2.5Ni.

 

Sebopeho sa lik'hemik'hale tsa tšepe ea weld(%):

C

Mn

Si

Ni

S

P

≤0.12

≤1.25

≤0.80

2.00 ~ 2,75

≤0.020

≤0.025

 

Mechine ea tšepe ea weld:

Ntho ea teko

Matla a tšepe

Mpa

Ho hlahisa matla

Mpa

Elongation

%

Boleng ba tšusumetso (J)

-60 ℃

Guaranteed

≥540

≥440

≥17

≥27

 

Diffusion hydrogen content of deposited metal: ≤6.0mL/100g (glycerin method) kapa ≤10mL/100g (mercury or gas chromatography method)

Tlhahlobo ea X-ray: Ke ea sehlopheng

 

Nako e khothalelitsoeng:

(mm)

Bophara ba molamu

3.2

4.0

5.0

(A)

Welding Current

90 ~ 120

140 ~ 180

180 ~ 210

 

Tlhokomeliso:

1. Electrode e tlameha ho behoa ka hora e le 1 ho 350 ℃ pele ho ts'ebetso ea welding;

2. Ho bohlokoa ho hloekisa mafome, sekala sa oli, metsi le litšila holim'a likarolo tsa ho tjheseletsa pele ho tjheseletsa.

 