AWS E7015-C2L Mocheso o Tlaase oa Tšepe Welding Electrode W107 Welding Rods Low Hydrogen Electrode ARC Stick Welding

Tlhaloso e Khutšoanyane:

W107 (AWS E7015-C2L) ke eleketrode ea tšepe e nang le mocheso o tlase e nang le lesela le tlase la hydrogen sodium..Sebelisa DCEP (electrode e nepahetseng hona joale) 'me e ka chesetsoa maemong ohle.Tšepe e kentsoeng e ntse e na le matla a ts'usumetso e ntle ho -100 ° C.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

Mocheso o tlase oa tšepe ea ho tjheseletsa Electrode

W107                                                     

GB/T E5015-C2L

AWS A5.5 E7015-C2L 

Tlhaloso: W107 ke eleketrode ea tšepe e nang le mocheso o tlase o nang le coat e tlase ea hydrogen sodium.Sebelisa DCEP (electrode e nepahetseng hona joale) 'me e ka chesetsoa maemong ohle.Tšepe e kentsoeng e ntse e na le matla a ts'usumetso e ntle ho -100 ° C. 

Kopo: E sebelisetsoa ho tjheseletsa tšepe ea mocheso o tlase joalo ka 3.5Ni.

 

Sebopeho sa lik'hemik'hale tsa tšepe ea weld(%):

C

Mn

Si

Ni

S

P

≤0.05

≤1.25

≤0.60

3.00 ~ 3,75

≤0.020

≤0.025

 

Mechine ea tšepe ea weld:

 

Ntho ea teko

 

Matla a tšepe

Mpa

 

Ho hlahisa matla

Mpa

Elongation%

Boleng ba tšusumetso (J) -100℃

 

Guaranteed

≥490

≥390

≥22

≥27

 

Diffusion hydrogen content of deposited metal: ≤4.0mL/100g (glycerin method) kapa ≤7.0mL/100g (mercury or gas chromatography method)

 

Tlhahlobo ea X-ray: Ke ea sehlopheng

 

Nako e khothalelitsoeng:

(mm)

Bophara ba molamu

2.0

2.5

3.2

4.0

5.0

(A)

Welding Current

Lilemo tse 40-70

70-90

90-130

140 ~ 180

180 ~ 240

 

 

Tlhokomeliso:

  1. Electrode e tlameha ho behoa bakeng sa hora e le 1 ho 350 ℃ pele ho ts'ebetso ea welding;
  2. Ho bohlokoa ho hloekisa mafome, sekala sa oli, metsi le litšila holim'a likarolo tsa tjheseletsa pele ho tjheseletsa;
  3. Leka ho sebelisa matla a mohala o monyane ha ho tjheseletsa, ho tjheseletsa ka mehala e mengata le ho tjheseletsa tse ngata.

 