Tyue Brand AWS ENiCrMo-4 Nickel le Nickel Based Alloy Welding Electrode, Best Arc Welding Rods, Welding Supplier

Tlhaloso e Khutšoanyane:

Ni327-4 (ENiCrMo-4) ke electrode e entsoeng ka nickel e nang le seaparo se tlaase sa hydrogen sodium.Sebelisa DCEP (electrode e nepahetseng hona joale).


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

Nickel le Nickel Alloy Welding Electrode

Ni327-4                                                     

GB/T ENi6276

AWS A5.11 ENCrMo-4

 

Tlhaloso: Ni327-4 ke electrode e thehiloeng ho nickel e nang le lesela le tlaase la hydrogen sodium.Sebelisa DCEP (electrode ea hona joale e tobilengntle).E na le ts'ebetso e ntle ea welding e nang le mollo o tsitsitseng oa arc, spatter e nyane, ho tlosa slag habonolo,

le weld e ntle.Thepa ea mechine ea tšepe e behiloeng e tsitsitse.

 

Kopo: E sebelisetsoa ho tjheseletsa li-alloys tsa nickel-chromium-molybdenum tse nang le carbon e tlaase, tse kang Hastelloy C276, ASTM B574, B575, B619, B622, B626, hape e ka sebelisoa bakeng sa ho tjheseletsa litšepe tse sa tšoaneng ka li-alloys tse ling tse thehiloeng ho nickel.

 

Sebopeho sa lik'hemik'hale tsa tšepe ea weld(%):

C

Mn

Si

Cr

Ni

Mo

≤0.02

≤1.0

≤0.2

14,5 ~ 16,5

≥50.0

15.0 ~ 17.0

W

Co

Fe

S

P

Tse ding

3.0 ~ 4.5

≤2.5

4.0 ~ 7.0

≤0.015

≤0.020

≤0.5

 

Mechine ea tšepe ea weld:

Ntho ea teko

Matla a tšepe

Mpa

Ho hlahisa matla

Mpa

Elongation

%

Guaranteed

≥690

≥400

≥22

 

Nako e khothalelitsoeng:

Bophara ba molamu

(mm)

2.5

3.2

4.0

Hona joale welding

(A)

60 ~ 90

70 ~ 110

90 ~ 150

 

Tlhokomeliso:

1. Electrode e tlameha ho behoa hora e le 1 ho pota 300 ℃ pele ho ts'ebetso ea welding.Leka ho sebelisa arc e khuts'oane ho cheselletsa;

2. Ke habohlokoa hore u hloekise mafome, oli, metsi le litšila holim'a likarolo tsa ho cheseletsa pele u cheselletsa.

3. Leka ho sebelisa matla a mohala o monyane ha ho tjheseletsa, ho etsa li-multi-layer le multi-pass welding.

 