Molemo ka ho Fetisisa oa Mofuta oa Tyue oa mofuta oa AWS A5.11 ENiCu-7 Li-electrode tsa Welding tse thehiloeng ho Nickel, Lithupa tsa Nickel Alloy Welding bakeng sa Arc Welding

Tlhaloso e Khutšoanyane:


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

Nickel le Nickel Alloy Welding Electrode

Ni207                                                     

GB/T ENi4060

AWS A5.11 ENCu-7

Tlhaloso: Ni207 ke Monel alloy electrode e nang le coating e tlase ea hydrogen sodium.Sebelisa DCEP (electrode e nepahetseng ea hona joale) 'me e na le ts'ebetso e ntle ea welding le ho hanyetsa crack.

Kopo: Bakeng sa welding Monel kapa litšepe tse sa tšoaneng.E ka boela ea sebelisoa bakeng sa overlay welding transition layer.

 

Sebopeho sa lik'hemik'hale tsa tšepe ea weld(%):

C

Mn

Fe

Si

Al

Ti

Cu

Nb

Ni

S

P

≤0.15

≤4.0

≤2.5

≤1.5

≤1.0

≤1.0

27.0 ~ 34.0

≤2.5

≥62.0

≤0.015

≤0.020

 

Mechine ea tšepe ea weld:

Ntho ea teko

Matla a tšepe

Mpa

Ho hlahisa matla

Mpa

Elongation

%

Guaranteed

≥480

≥200

≥27

 

Nako e khothalelitsoeng:

Bophara ba molamu

(mm)

3.2

4.0

Hona joale welding

(A)

90 ~ 110

110 ~ 150

 

Tlhokomeliso:

1. Electrode e lokela ho apehoa lihora tse 2 ho pota 300 ℃ pele ho ts'ebetso ea welding;

2. Ke habohlokoa hore u hloekise mafome, oli, metsi le litšila holim'a likarolo tsa ho cheseletsa pele u cheselletsa.Leka ho sebelisa arc e khuts'oane ho cheselletsa.

 