Tlhaloso e Khutšoanyane:

AWS E6011elektrode ea ho tjheseletsake mofuta oa potassium ea cellulose, e sebelisetsoang ho tjheseletsa ka ho otloloha. Ka bobeli bakeng sa ho tjheseletsa ka AC le DC.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Kopo
Lithupa tsa ho tjheseletsa AWS E6011 e loketse meaho ea likepe tsa ho tjheseletsa tse kang mehaho le marokho, litanka tsa polokelo, liphaephe le lisebelisoa tsa likepe tsa khatello.

AWS E6011elektrode ea ho tjheseletsake mofuta oa potassium ea cellulose, e sebelisetsoang ho tjheseletsa ka ho otloloha. Ka bobeli bakeng sa ho tjheseletsa ka AC le DC. E amohela theknoloji e tsoetseng pele ea kantle ho naha 'me e na le litšobotsi tse ntle tsa theknoloji ea ho tjheseletsa. Bolelele ba ARC bo lokela ho laoloa ka tekanyo e loketseng. Ha se ho tjheseletsa ka ho feletseng le ho tjheseletsa ka sekoahelo.

Sebopeho sa Lik'hemik'hale (%)
C Mn Si S P
≤0.2 0.3-0.6 ≤0.22 ≤0.03 ≤0.04
Matlotlo a Mekaniki a Tšepe e Lahliloeng
Ntho ea Teko Rm (N/mm2) Rel (N/mm2) A (%) KV2(J) 0℃
Boleng ba Tiisetso ≥420 ≥330 ≥22 ≥47
Sephetho se Akaretsang 485 380 24 86
Referense ea Hona Joale (DC)
Bophara φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Amperage 40 ~ 70 50 ~ 90 90 ~ 130 130 ~ 210 170 ~ 230

MOFUTA OA HONA JOALE: Electrode ea Hona Joale e Khethehileng (DCEP) kapa AC

Mekhoa ea ho tjheseletsa e khothaletsoang:

Bolelele ba Arc – Bolelele bo tloaelehileng (1/8” ho isa ho 1/4”)

Sephara - Lula ka pele ho letangoana la metsi 'me u sebelise motsamao o monyenyane oa ho shapa

E otlolohileng - Electrode ea Angle hanyane ho ea holimo poleiting

Holimo ka ho Otloloha – Mokhoa oa ho shapa kapa ho loha hanyane

Ho theosa ka ho otloloha - Sebelisa amperage e phahameng le leeto le potlakileng, u lule u le ka pele ho letangoana la metsi

Holimo - Lula ka pele ho letamo 'me u sebelise motsamao o monyenyane oa ho shapa

Tlhokomeliso:
1. Ho bonolo ho e pepesetsa mongobo, ka kopo e boloke e omme.
2. E hloka ho futhumatsoa ha sephutheloana se robeha kapa mongobo o monya, mocheso oa ho futhumatsa o lokela ho ba pakeng tsa 70C ho isa ho 80C, nako ea ho futhumatsa e lokela ho ba hora e 0.5 ho isa ho e 1.
3. Ha o sebedisa di-electrode tsa ho tjheseletsa tsa 5.0mm, ho molemo ho sebedisa matla a ho tjheseletsa a phahameng, a motlakase o tlase, e le ho ntlafatsa tshebetso ya ho tjheseletsa.