Elektrode ea tšepe ea khabone ea TYUE E7018

Tlhaloso e Khutšoanyane:

Elektrode ea tšepe ea carbon e koahetsoeng ka phofo ea hydrogen potassium.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Tlhophiso:

AWS A5.1 E7018

ISO 2560-B-E4918A

GB/T 5117 E5018

Liropo tsa ho Welding AWS E7018 ke electrode ea tšepe ea carbon e koahetsoeng ka phofo ea hydrogen potassium e nang le hydrogen e tlase. Lerōle la tšepe le koahetsoeng le eketsa sekhahla sa depositi. E na le ts'ebeliso e ntle haholo e e lumellang ho ba le arc e tsitsitseng, ho fafatsa hanyane, ho tlosa slag ho bonolo ebile ho tjheseletsa maemong 'ohle. Tšepe e kentsoeng e na le thepa e ntle ea mechini e fanang ka ho tiea ho hotle haholo mochesong o tlase.

Sebopeho sa lik'hemik'hale (%)
Sebopeho sa Lik'hemik'hale

C

Mn

Si

S

P

Boleng ba Tiisetso

≤0.12

≤1.60

≤0.75

≤0.035

≤0.040

Sephetho se Akaretsang

0.089

1.2

0.38

0.028

0.04

Thepa ea mechini ea tšepe e bolokiloeng
Ntho ea Teko

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) -30°C

Boleng ba Tiisetso

≥490

≥400

≥20

≥27

Sephetho se Akaretsang

515

430

32

156

Hona joale ea litšupiso (DC)

Bophara

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

60 ~ 100

80 ~ 140

110 ~ 210

160 ~ 230

Boemo ba ho tjheseletsa:

PA, PB, PC, PD, PE, PF

Lintlha:
1. Electrode e tlameha ho futhumatsoa mochesong oa 350°C ka hora e le 'ngoe. Chesa thupa neng kapa neng ha e sebelisoa.
2. Litšila tse kang mafome, matheba a oli le mongobo li lokela ho tlosoa mosebetsing.
3. Ho hlokahala seqha se sekgutshwane ho etsa tjheseletso. Tsela e moqotetsane ya tjheseletso e a kgethwa.

 

Tlhokomeliso:

  1. Telectrode e lokela ho omisoa hape ka 350℃-380℃hora e le 'ngoe pele ho tjheseletsa.
  2. Tphomolo, oli, metsi le litšila tse ling tsa sebaka sa ho tjheseletsa li lokela ho tlosoa pele ho tjheseletsa.