Hardfacing Welding Electrode DIN 8555 (E9-UM-250-KR) Surfacing Welding Electrode, Stick Welding Rods

Tlhaloso e Khutšoanyane:

DIN 8555 (E9-UM-250-KR) ke elektrode e Khethehileng e nang le lisebelisoa tse ntle tsa welding le mochini.Austenite- Ferrites weld tšepe.Maemo a phahameng a matla le khanyetso e phahameng ea crack.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

Hardfacing WeldingElectrode

Maemo: DIN 8555 (E9-UM-250-KR)

Nomoro ea mofuta: TY-C65

 

Tlhaloso & Tšebeliso:   

· Electrode e khethehileng e nang le welding e nepahetseng le thepa ea mochini.

· Austenite- Ferrites weld tšepe.Maemo a phahameng a matla le khanyetso e phahameng ea crack.

· Haholo-holo e loketse ho kopanngoa ka litšepe tse thata haholo, ha ho etsoa litlhoko tse phahameng ka ho fetisisa holim'a seam.

· Ho hanyetsa crack ho hoholo ha o kopanya litšepe tsa motsoali tse thata ho cheseha, joalo ka litšepe tsa austenitic le ferritic, litšepe tse phahameng tsa manganese tse nang le litšepe tse kopantsoeng le tse sa tsoeng, tse pholileng mocheso le litšepe tsa lisebelisoa.Likopo tsa tokiso le tlhokomelo ea mochini le likarolo tsa koloi hammoho le tokisong ea lisebelisoa.

· Joalo ka mosamo lera holim'a lisebelisoa tsena e boetse e ka tsela e loketseng loketseng.

 

 

Motsoako oa lik'hemik'hale oa tšepe e behiloeng (%):

 

C

Si

Mn

P

S

Cr

Ni

Mo

N

Fe

DIN

-

0.15

-

0.90

0.50

2.50

-

0.04

-

0.03

28.0

32.0

8.0

10.0

-

-

Bal.

E tloaelehileng

0.1

1.0

1.0

≤0.035

≤0.025

29.0

9.0

≤0.75

0.10

Bal.

 

Ho thatafala ha tšepe e behiloeng:

Ho hlahisa matla

Mpa

Matla a tšepe

Mpa

Elongation

A(%)

Ho thatafala Joalo ka Welded

(HB)

620

800

22

240

 

Litšobotsi tse Akaretsang:

· Microstructure Austenite + Ferrite

· Machinability Excellent

· Preheating Preheating ea likarolo tse teteaneng tsa ferritic ho isa ho 150-150 ℃

· Redrying Redry bakeng sa 2 h ho 150-200 ℃ pele o sebelisoa.

 

 