D256 (B-80) Hardfacing Welding Electrode, Surfacing Welding Rod, Arc Welding Stick

Tlhaloso e Khutšoanyane:

Electrode ea mantlha e behang tšepe ea manganese ea austenitic, e thatafalang ka ho senyeha ho batang, e sebetsang ho litšepe tsa sebopeho se tšoanang le likarolong tse nang le ts'oaetso e matla le makhopho a mahareng.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

Hardfacing Welding Stick ElectrodeRODO P

RODO PARA RECUBRIMIENTO MOTŠIRELETSO

Nomoro ea mofuta: D256B-80)

Deposited Metal Analysis (Maemo a tloaelehileng)

C

1.2%

Mn

13.0%

Si

0.5%

Ni

3.0%

 

Litšobotsi:

Electrode ea mantlha e behang tšepe ea manganese ea austenitic, e thatafalang ka ho senyeha ho batang, e sebetsang ho litšepe tsa sebopeho se tšoanang le likarolong tse nang le ts'oaetso e matla le makhopho a mahareng.E loketse ho hlaphoheloa, ho roala le ho lokisa likarolo tsa tšepe tsa austenitic Mn, likarolo le likotoana tsa mechine e boima.

 

Thepa ea Mechini:Boima ba 200-250 HB BRINELL ho depositi, 300-400 HB Brinell

ka mor'a mosebetsi o batang oa ho thatafala.

 

Maemo a Welding:E bataletseng, e Tshekaletseng, Kahodimo, E Emeng Hodimo.

 

Hona joale le Polarity:

Bakeng sa maqhubu a feto-fetohang kapa a tobileng

eleketrode ho palo e ntle

ho mm

ø ka

Amperage

3.20

1/8

110-130

4.00

5/32

140-160

5.00

2/16

180-230

 

Lisebelisoa: • Ho tlatsa litšepe tsa Manganese.

• Ho tsosolosoa ha meno le libakete tsa excavator.

• Ho tšela le lipelo tsa rails.

• Masilo a liminerale le lihamore.

• Ka ho otla boima ba eona bo eketseha ho 350 - 400 HB.

• Ha o aha bocha kapa o acoa bocha, sebelisa AG AR-91 e le motheo.

• Ha mocheso o ka holimo ho 300 OC, Mn steels

Ba qala ho lahleheloa ke boima.Li-laces li khothaletsoa

tlolela, bonyane bophara le amperage ho khoneha.

 

 

BOLEMO: 350mm.

Boima ka Lebokose: 20 kg / 44 lbs.

 

Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka 2000. Re se re ntse re etsa tlhahiso eaelectrode ea ho tjheseletsas, melamu ea ho cheselletsa, le lisebelisoa tsa ho cheselletsa ka lilemo tse fetang 20.

Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa tšepe e sa hloekangelectrode ea ho tjheseletsas, carbon steel welding electrode, low alloy welding electrode, surfacing welding electrode, nickel & cobalt alloy welding electrode, mild steel & low alloy wires, stainless steel welding wires, gas-shielded flux cored wires, aluminium welding wires, submerged arc wires. .lithapo, lithapo tsa nickel & cobalt alloy welding, lithapo tsa tšepe tsa koporo, lithapo tsa welding tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tsa carbon gouging, le lisebelisoa tse ling tsa welding & consumables.

 

 

 

 


  • E fetileng:
  • E 'ngoe: