Tlhaloso e Khutšoanyane:

EC410NiMo ke terata e nang le mothapo wa tshepe e sa ruseng ya martensitic e nang le motswako wa dikhemikhale o nang le 11.0 – 12.5% ​​Cr, 4.0 – 5.0% Ni, le 0.40 – 0.70% Mo.

Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Tekanyetso e Tšoanang

GB/T 17853-2018 TS410NiMo-FC11

AWS A5.22M-2012 E410NiMoT1-1

Tekanyo e Lekanang: 13Cr-4Ni (EN1.4313/UNS S41500)

Tlhaloso

EC410NiMo ke terata ea tšepe e sa hloekang ea martensitic e nang le motsoako oa lik'hemik'hale o nang le 11.0 – 12.5% ​​Cr, 4.0 – 5.0% Ni, le 0.40 – 0.70% Mo. E loketse maemo ohle.ho tjheseletsa arc e nang le mothapo o phallang(FCAW) e nang le arc e tsitsitseng, ho fafatsa ho fokolang, le ho arohana ho babatsehang ha slag. Tšepe e kentsoeng e na le khanyetso e ntle ea ho tsofala, khanyetso ea ho petsoha, le thepa ea mechini. Ho futhumatsoa esale pele ho 150 - 260℃ hoa khothaletsoa, ​​'me kalafo ea mocheso oa kamora ho weld (PWHT) ho 590 ~ 620℃ ka hora e le' ngoe (e lateloe ke ho pholisa moea, AC) ea hlokahala kamora ho weld.

Kopo

E loketse ho tjheseletsa tšepe e entsoeng ka ASTM CA6NM le litšepe tsa letoto la 13%Cr – 4%Ni. E sebelisoa bakeng sa ho lokisa lireile tsa crane, lirolara tsa khatiso, li-shaft tsa tšepe, likarolo tsa motlakase oa metsi tse aparetsoeng ke cavitation, le likarolo tsa sebopeho tse hlokang ho ts'oaroa le ho hanyetsa ho tsofala.

Sebopeho sa Lik'hemik'hale sa Tšepe e Welded (%)

Karolo C Cr Ni Mo Mn Si P S Cu
Tlhokahalo ≤0.06 11.0-12.5 4.0-5.0 0.40-0.70 ≤1.00 ≤1.00 ≤0.040 ≤0.030 ≤0.75
Sephetho sa Teko 0.02 12.3 4.65 0.54 0.59 0.33 0.023 0.01 0.01

Matlotlo a Mekaniki a Tšepe e Lahliloeng

Lebitso la Teko Matla a ho Tenyetseha (MPa) Ho lelefatsa% X-ray Teko ea Tšusumetso(+20℃)J Bothata HB Haedrojene e qhalanang (ml/100g)
Tlhokahalo ≥760 ≥15 Sehlopha sa I – – ≤5
Sephetho sa Teko 845 19 Sehlopha sa I 60-90 250-310 ≤5

 

Paramethara ea ho tjheseletsa e khothaletsoang

Mohloli oa Matla: DC Reverse (DC-)

Bophara ba terata le Hona Joale:

Khoeli e Khothaletsoang:

Bophara ba molamu (mm) 3.2 4.0 5.0
Ho tjheseletsa Hona Joale (A) 80-120 120-160 150-190

Tsebiso

1. Baka electrode ho 300℃ hora pele o e sebedisa ho tlosa mongobo.

2. Hloekisa mafome, oli le mongobo holim'a tšepe e ka tlase; sebelisa ts'ebetso e khutšoanyane ea arc bakeng sa lifaha tse tšesaane tsa weld.

3. PWHT e lokela ho etsoa hang ka mora ho tjheseletsa ho qoba ho robeha ha lehare.

 

 