Elektrode ea ho tjheseletsa ea E410NiMo-15

Tlhaloso e Khutšoanyane:

E410NiMo-15 ke electrode ea ho tjheseletsa ea tšepe e sa hloekang ea martensitic e nang le sodium e nang le haedrojene e tlase ea 11.0-12.5% ​​Cr, 4.0-5.0 Ni, le 0.40-0.70% Mo.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Tekanyetso e Tšoanang

GB/T 983-2012 E410NiMo-15

AWS A5.4M-2012 E410NiMo-15

Thepa e Lekanang:1.4317 GX4CrNi13-4,1.4313 X3CrNiMo13-4,1.4407 GX5CrNiMo13-4,1.4414 GX4CrNiMo13-4,ACI Gr. CA6NM,UNS S41500

Tlhaloso

E410NiMo-15 ke electrode ea ho tjheseletsa tšepe e sa hloekang ea martensitic e nang le sekoahelo sa sodium se nang le haeterojene e tlase, e nang le 11.0-12.5% ​​Cr, 4.0-5.0% Ni, le 0.40-0.70% Mo. E loketse ho tjheseletsa tšepe e sirelelitsoeng (SMAW) e nang le arc e tsitsitseng, ho fafatsa ho fokolang, le ho arohana ho babatsehang ha slag. Tšepe e kentsoeng e fana ka matla a phahameng, ho hanyetsa mafome hantle, le ho hanyetsa ho petsoha. Ho futhumatsoa ho khothaletsoa bakeng sa mesebetsi e teteaneng, 'me kalafo ea mocheso oa kamora ho tjheseletsa (PWHT) ho 580~620℃ (lihora tse 1-2, ho pholisa moea, AC) ea hlokahala.

Kopo

E loketse ho tjheseletsa tšepe e entsoeng ka ASTM CA6NM, litšepe tsa letoto la 13%Cr-4%Ni (mohlala, Cr13Ni4Mo,Cr13Ni5Mo), le litšepe tse tšoanang tse sa hloekang tsa martensitic. Litšebeliso tse tloaelehileng li kenyelletsa ho tjheseletsa tokiso ea li-turbine tsa hydropower runners, li-valve body, liphaephe tse nang le khatello e phahameng, le bokaholimo ba likarolo tse aparoang ke cavitation. E boetse e sebelisoa bakeng sa tokiso ea lifahleho tse thata tsa likarolo tse sa tsofaleng joalo ka lirolo tsa crusher le li-casing tsa pompo.

Sebopeho sa Lik'hemik'hale sa Tšepe e Weld(%)

Karolo C Mn Si P S Cr Ni Mo Cu
Tlhokahalo ≤0.06 ≤1.0 ≤0.90 ≤0.04 ≤0.03 11.0-12.5 4.0-5.0 0.40-0.70 ≤0.75
Sephetho sa Teko 0.029 0.7 0.32 0.028 0.01 12.26 4.50 0.55 0.01

Matlotlo a Mekaniki a Tšepe e Lahliloeng

Lebitso la Teko Matla a ho Tenyetseha (Mpa) Ho lelefatsa% X-ray Teko ea Tšusumetso, (+20℃)J Bothata HB Haedrojene e qhalanang (ml/100g)
Tlhokahalo ≥760 ≥15 Sehlopha sa I – – ≤5
Sephetho sa Teko 845 19 Sehlopha sa I 60-90 250-310 ≤5

Liparamitha tse khothaletsoang tsa ho tjheseletsa

Mohloli oa Motlakase: DC Reserve (DC-)

Khothaletso ea Hona Joale

Bophara ba molamu (mm) 3.2 4.0 5.0
Ho tjheseletsa Hona Joale (A) 80-120 120-160 150-190

Tsebiso:

1. Baka electrode ho 300℃ hora pele o e sebedisa ho tlosa mongobo.
2. Hloekisa mafome, oli le mongobo holim'a tšepe e ka tlase; sebelisa ts'ebetso e khutšoanyane ea arc bakeng sa lifaha tse tšesaane tsa weld.
3. PWHT e lokela ho etsoa hang ka mora ho tjheseletsa ho qoba ho robeha ha lehare.