AFE312-16 (AWS E312-16) ke electrode ea tšepe e sa hloekang ea Cr29Ni9 e nang le sekoahelo sa titanium-calcium.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Electrode ea ho tjheseletsa ea Tšepe e sa Khaotseng

AF312-16

GB/T E312-16

AWS A5.4 E312-16

Tlhaloso: AFE312-16 ke electrode ea tšepe e sa hloekang ea Cr29Ni9 e nang le sekoahelo sa titanium-calcium. E ka sebelisoa bakeng sa AC le DC ka ts'ebetso e ntle ea ts'ebetso. Hobane e na le molybdenum le naetrojene, 'me litaba tsa khabone li tlase haholo, tšepe e bolokiloeng e na le khanyetso e ntle ea mapetso le khanyetso ea mafome, haholo-holo khanyetso ea mafome ea khatello.

Tšebeliso: E sebelisetsoa ho tjheseletsa tšepe e sa ruseng ea letoto la 29-9, tšepe e entsoeng ka tšepe le tšepe e sa tšoaneng, hammoho le ho tjheseletsa thepa e ka bang le mapetso le masoba.

 

Sebopeho sa lik'hemik'hale sa tšepe e welded (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.15

0.5 ~ 2.5

≤0.90

28.0 ~ 32.0

8.0 ~ 10.5

≤0.75

≤0.75

≤0.030

≤0.040

 

 

Litšobotsi tsa mechini tsa tšepe e welded:

Ntho ea teko

 Matla a tšepe

Mpa

Ho lelefatsa

%

E tiiselitsoe

≥660

≥22

 

Khoeli e khothaletsoang:

Bophara ba molamu

()mm)

2.5

3.2

4.0

5.0

ho tjheseletsa hona joale

()A)

50 ~ 80

80 ~ 110

100 ~ 150

140 ~ 180

 

Tsebiso:

1. Electrode e lokela ho besoa hora e le 'ngoe mochesong o ka bang 250℃ pele ho ts'ebetso ea ho tjheseletsa.

 

Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka selemo sa 2000. Re 'nile ra kopanela tlhahisong ea li-electrode tsa ho tjheseletsa, lithupa tsa ho tjheseletsa le lisebelisoa tse sebelisoang tsa ho tjheseletsa ka lilemo tse fetang 20.

Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa li-electrode tsa tšepe e sa hloekang, li-electrode tsa tšepe ea khabone, li-electrode tsa ho tjheseletsa tse nang le alloy e tlase, li-electrode tsa ho tjheseletsa tse holim'a metsi, li-electrode tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tse nang le alloy e bobebe le e nang le alloy e tlase, lithapo tsa ho tjheseletsa tse nang le alloy e sirelelitsoeng ke khase, lithapo tsa ho tjheseletsa tsa aluminium, ho tjheseletsa ka har'a arc e ka tlas'a metsi. lithapo, lithapo tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tsa koporo, lithapo tsa ho tjheseletsa tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tse sehang khabone, le lisebelisoa tse ling tsa ho tjheseletsa le tse sebelisoang.

 


  • E fetileng:
  • E 'ngoe: