Tig le Mig Wire A5.28 ER80S-D2, Metals ea Filler ea tšepe e tlase ea alloy bakeng sa Welding ea Gas Shielded Arc

Tlhaloso e Khutšoanyane:

ER80S-D2 ke terata e tiileng ea tšepe e bonolo e sebelisoang maemong ao porosity e leng bothata kapa ha o tlameha ho hanyetsa lintho tse nang le sebabole se phahameng kapa khabone tšepeng ea hau ea motheo.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

A5.28 ER80S-D2, Metals ea Tlatsi ea tšepe e tlase ea alloy bakeng sa Welding ea Arc e Shielded

ER80S-D2 ke terata e tiileng ea tšepe e bonolo e sebelisoang maemong ao porosity e leng bothata kapa ha o tlameha ho hanyetsa lintho tse nang le sebabole se phahameng kapa khabone tšepeng ea hau ea motheo.E na le maemo a phahameng a manganese le silicon ho fana ka metsi a matle hammoho le mafome a matle le mamello ea sekhahla.

Lits'ebetso tse Tloaelehileng: lits'ebetso tsa boleng ba x-ray, li-welld tse matla haholo, liboiler tsa mouoane, litanka tsa khatello, lipeipi tsa khase, phapanyetsano ea mocheso, indasteri ea petrochemical.

Sehlopha sa AWS: ER80S-D2 Setifikeiti: AWS A5.28/A5.28M:2005
motsoako: ER80S-D2 AWS/ASME SFA A5.28

 

Boemo ba Welding: F, V, OH, H Hona joale:
GMAW-DCEP

 

Matla a Tensile, kpsi: 80 mets
Kotulo e Matla, kpsi: 68 mets
Elongation %: 17 mets

Tlhōrō ea Wire Chemistry ho ea ka AWS A5.28 (litekanyetso tse le 'ngoe ke tse phahameng)

C Mn Si P S Ni Mo Cu Tse ding
0.07-0.12 1.60-2.10 0.50-0,80 0.025 0.025 0.15 0.40-0,60 0.50 0.50
Mefuta e tloaelehileng ea Welding
Diameter Tshebetso Volt Amps Tšireletso ea Khase
in (mm)
.035 (0.9) GMAW 28-32 165-200 Ho fetisoa ha spray 98% Argon / 2% Oxygen
.045 (1.2) GMAW 30-34 180-220 Ho fetisoa ha spray 98% Argon / 2% Oxygen
1/16 (1.6) GMAW 30-34 230-260 Ho fetisoa ha spray 98% Argon / 2% Oxygen
.035 (0.9) GMAW 22-25 100-140 Phetisetso e Khutšoanyane ea Potoloho 90% Helium/ 75% Argon / 25% CO2
.045 (1.2) GMAW 23-26 120-150 Phetisetso e Khutšoanyane ea Potoloho 90% Helium/ 75% Argon / 25% CO2
1/16 (1.6) GMAW 23-26 160-200 Phetisetso e Khutšoanyane ea Potoloho 90% Helium/ 75% Argon / 25% CO2
1/16 (1.6) GTAW 12-15 100-125 100% Argon
3/32 (2.4) GTAW 15-20 125-175 100% Argon
1/8 (3.2) GTAW 15-20 175-250 100% Argon

 