AWS EN-1 Pure Nickel Welding Electrode Ni102 Nickel Alloy Electrodes Stick Welding Rods bakeng sa Arc Welding

Tlhaloso e Khutšoanyane:

Ni102 (AWS ENi-1) ke electrode e hloekileng ea nickel e nang le titanium-calcium coating.E ka sebelisoa bakeng sa tjheseletsa ea maemo ohle ka AC le DC.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

Alloy ea Nickel le NickelWeldingElectrode

Ni102                                                     

GB/T EN2061

AWS A5.11 EN-1

Tlhaloso: Ni102 ke electrode e hloekileng ea nickel e nang le titanium-calcium coating.E ka sebelisoa bakeng sa tjheseletsa ea maemo ohle ka AC le DC.Tšepe e kentsoeng e na le thepa e ntle ea mochini, ho hanyetsa mocheso le ho hanyetsa kutu.

Kopo: E sebelisetsoa ho tjheseletsa nickel e hloekileng (UNS N02200 kapa N02201) lisebelisoa tsa tšepe le tse entsoeng ka tšepe, ho cheselletsa tšepe e entsoeng ka nickel, holim'a tšepe le ho cheselletsa tšepe e sa tšoaneng.

 

Sebopeho sa lik'hemik'hale tsa tšepe ea weld(%):

C

Mn

Fe

P

S

Si

Al

Ti

Ni

Cu

Tse ding

≤0.10

≤0.7

≤0.7

≤0.020

≤0.015

≤1.2

≤1.0

1.0 ~ 4.0

≥92.0

≤0.2

≤0.5

 

Mechine ea tšepe ea weld:

Ntho ea teko

Matla a tšepe

Mpa

Ho hlahisa matla

Mpa

Elongation

%

Guaranteed

≥410

≥200

≥18

 

Nako e khothalelitsoeng:

Bophara ba molamu

(mm)

2.5

3.2

4.0

Hona joale welding

(A)

Lilemo tse 50-80

80 ~ 120

130 ~ 170

 

Tlhokomeliso:

1. Electrode e tlameha ho behoa bakeng sa hora e le 1 ho pota 350 ℃ pele ho ts'ebetso ea welding;

2. Ke habohlokoa hore u hloekise mafome, oli, metsi le litšila holim'a likarolo tsa ho cheseletsa pele u cheselletsa.

 