AWS A5.18 ER70S-6 Carbon Steel Welding Wire Filler Metals for Gas Shielded Arc Welding, Solid Wire Wire

Tlhaloso e Khutšoanyane:

ER70S6 ke terata e bonolo ea tšepe ea tšepe e nang le maemo a holimo a manganese le silicon ho feta limaraka tse ling tse tloaelehileng tsa terata ea MIG ho isa lihlahisoa tsa boleng bo holimo ha li sebelisoa holim'a tšepe e litšila, e mafura kapa e mafome.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

ER70S6 ke terata e bonolo ea tšepe ea tšepe e nang le maemo a holimo a manganese le silicon ho feta limaraka tse ling tse tloaelehileng tsa terata ea MIG ho isa lihlahisoa tsa boleng bo holimo ha li sebelisoa holim'a tšepe e litšila, e mafura kapa e mafome.Likahare tse phahameng tsa silicon li eketsa metsi a letamo la weld, kahoo li etsa ponahalo ea lifaha tse boreleli 'me li baka ho sila ho fokolang ka morao.Mohala ona o entsoe ka mokhoa oa ho fana ka litšepe tsa boleng ba x-ray tse se nang porosity ka matla a phahameng ka ho fetesisa (joalo ka ha a cheselitsoe) ho feta lithapo tsohle tsa tšepe tsa carbon.

Likopo tse Tloaelehileng: likopo tse akaretsang tsa mabenkele tse nang le lipoleiti tse sa lekanang hantle kapa tse mafome, tse mafura;li-castings tsa tšepe kapa tsa forging salvage;merero ea lapeng;letlapa tšepe;litanka;mosebetsi oa kaho

Sehlopha sa AWS: ER70S6

Setifikeiti: AWS A5.18/A5.18M:2005

motsoako: ER70S6

ASME SFA A5.18

Boemo ba Welding: F, V, OH, H

Hona joale: DCEP

Matla a Tensile, kpsi:

70

Kotulo e Matla, kpsi:

58

Elong ka 2”%:

22

Tlhōrō ea Wire Chemistry ho ea ka AWS A5.18 (litekanyetso tse le 'ngoe ke tse phahameng)

C

Mn

Si

P

S

Ni

Cr

Mo

V

Cu

0.06-0.15

1.40-1,85

0.80-1.15

0.025

0.035

0.15

0.15

0.15

0.03

0.50

Mefuta e tloaelehileng ea Welding

Diameter

Tshebetso

Volt

Lebelo la ho Eta

Amps

Tšireletso ea Khase

in

(mm)

(ipm)

.035

(0.9)

GMAW

23-26

11-22

160-300

Spray Transfer 98% Argon+2% Oxygen

.045

(1.2)

GMAW

23-29

12-21

170-375

Spray Transfer 98% Argon+2% Oxygen

1/16

(1.6)

GMAW

25-31

9-19

275-475

Spray Transfer 98% Argon+2% Oxygen

.023

GMAW

14-19

10-15

30-85

Phetisetso e Khutšoane ea Potoloho 98% Argon + 2% Oksijene

.030

(0.8)

GMAW

15-20

12-24

40-130

Phetisetso e Khutšoane ea Potoloho 98% Argon + 2% Oksijene

.035

(0.9)

GMAW

16-25

11-40

60-235

Phetisetso e Khutšoane ea Potoloho 98% Argon + 2% Oksijene

.045

(1.14)

GMAW

18-23

12-22

90-290

Phetisetso e Khutšoane ea Potoloho 98% Argon + 2% Oksijene

.035

(0.9)

GTAW

12-15

N/A

60-100

100% Argon

.045

(1.14)

GTAW

13-16

N/A

70-120

100% Argon

1/16

(1.6)

GTAW

12

N/A

100-160

100% Argon

1/16- 3/32

(1.6)-(2.4)

GTAW

12

N/A

120-250

100% Argon

1/8

(3.2)

GTAW

12

N/A

150-300

100% Argon