Terata ea ho Wellisa ea Arc e qoelitsoeng ka EM12K
Sehlopha sa AWS A5.17 EM12K
Terata ea arc e ka tlas'a metsi ea EM12K e na le maemo a holimo a khabone, manganese le silicon ho feta EL12. Keketseho ea khabone e fa terata ena matla a ho tensile a maholo, ha keketseho ea manganese le silicon e hlahisa litšobotsi tse ntlafetseng tsa deoxidation. EM12K e tla hlahisa li-weld deposits tse nang le masoba a fokolang esita le holim'a mafome le sekala sa tšilo tse ka bang teng tšepeng ea motheo. Terata ena e sebelisoa haholo bakeng sa li-weld tsa single pass butt le fillet holim'a lipoleiti tsa tšepe tse bobebe le tse tlase tse fihlang ho 1/2” botenya. Litšebeliso tse tobileng haholoanyane li tla kenyelletsa ASTM A537, A283, Grades A, B, kapa C. Kaha EM12K e fana ka li-weld tsa matla a holimo/tse tlase tse nang le masoba holim'a li-alloy tse ngata tsa tšepe, ke terata ea arc e ka tlas'a metsi e theko e tlaase ka ho fetisisa ho e boloka.
KHEMISI EA TŠEPE E TLWAELEHILENG EA HO WELDA %
| C | 0.150 |
| Mn | 1.100 |
| Si | 0.250 |
| P | 0.017 |
| S | 0.024 |
Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka selemo sa 2000. Re 'nile ra kopanela tlhahisong ea li-electrode tsa ho tjheseletsa, lithupa tsa ho tjheseletsa le lisebelisoa tse sebelisoang tsa ho tjheseletsa ka lilemo tse fetang 20.
Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa li-electrode tsa tšepe e sa hloekang, li-electrode tsa tšepe ea khabone, li-electrode tsa ho tjheseletsa tse nang le alloy e tlase, li-electrode tsa ho tjheseletsa tse holim'a metsi, li-electrode tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tse nang le alloy e bobebe le e nang le alloy e tlase, lithapo tsa ho tjheseletsa tse nang le alloy e sirelelitsoeng ke khase, lithapo tsa ho tjheseletsa tsa aluminium, ho tjheseletsa ka har'a arc e ka tlas'a metsi. lithapo, lithapo tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tsa koporo, lithapo tsa ho tjheseletsa tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tse sehang khabone, le lisebelisoa tse ling tsa ho tjheseletsa le tse sebelisoang.