Lithupa tsa welding AWS A5.1 E6013 (J421)

Tlhaloso e Khutšoanyane:

tjheseletsa melamu AWS A5.1 E6013 (J421) ke a loketse bakeng sa tjheseletsa tsa sebopeho tlaase k'habone tšepe, haholo-holo bakeng sa tjheseletsa ea tšesaane poleiti tšepe le khutšoanyane discountinuous tjheseletsa le tlhokahalo ea ho feta boreleli tjheseletsa.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

tjheseletsa melamu AWS A5.1 E6013 (J421) ke a loketse bakeng sa tjheseletsa tsa sebopeho tlaase k'habone tšepe, haholo-holo bakeng sa tjheseletsa ea tšesaane poleiti tšepe le khutšoanyane discountinuous tjheseletsa le tlhokahalo ea ho feta boreleli tjheseletsa.

Lihlopha:

ISO 2560-A-E35 0 RA 12

AWS A5.1: E6013

GB/T 5117 E4313

Litšobotsi:

AWS A5.1 E6013 (J421) ke rutile mofuta electrode.E ka ba mohloli oa matla oa AC & DC 'me e ka ba bakeng sa maemo ohle.E na le ts'ebetso e babatsehang ea ho tjheseletsa e le arc e tsitsitseng, spatter e nyenyane, ho tlosoa ha slag habonolo le ho busa-bokhoni joalo-joalo Rutile-cellulosic electrode e nang le bokhoni bo botle ba weld maemong ohle ho kenyeletsa le ho theosa fatše.Bokhoni bo botle ba ho koala lekhalo le bokhoni ba ho otla arc.Bakeng sa li-welding tsa tack le li-fit ups tsa mojaro.Sepheo se akaretsang sa indasteri le khoebo, kopano le ho cheselletsa mabenkele.

Tlhokomeliso:

Ka kakaretso, ha ho hlokahale hore o omise electrode hape pele o tjheseletsa.Ha e angoa ke mongobo, e lokela ho omisa hape ho 150 ℃-170 ℃ bakeng sa hora ea 0.5-1.

Boemo ba Welding:

PA, PB, PC, PD, PE, PF

AWS A5.1 E6013 e loketse meaho ea tjheseletsa e entsoeng ka tšepe e tlase ea khabone, e sebetsa hantle haholo ka lipoleiti tsa tšepe tse tšesaane le tse nyane hape e na le ts'ebetso e ntle haholo maemong a hlokang ponahalo e ntle le e hloekileng ea lifaha.

Motsoako oa Lik'hemik'hale oa All Weld Metal: (%)

Sebopeho sa Lik'hemik'hale

C

Mn

Si

S

P

Ni

Cr

Mo

V

Litlhoko

≤0.10

0.32-0,55

≤0.30

≤0.030

≤0.035

≤0.30

≤0.20

≤0.30

≤0.08

Liphetho tse Tloaelehileng

0.08

0.37

0.18

0.020

0.025

0.030

0.035

0.005

0.004

Mechanical Properties of Deposited Metal

Ntho ea Teko

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) 0℃

Litlhoko

440-560

≥355

≥22

≥47

Liphetho tse Tloaelehileng

500

430

27

80

Reference Current (DC)

Diameter

φ2.0

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

Lilemo tse 40-70

50 ~ 90

80 ~ 130

150 ~ 210

180 ~ 240

Tlhahlobo ea X-Ray Radiographic:

Boemo Ⅱ


  • E fetileng: