Nickel Alloy Welding Wire ERNi-1 Nickel Tig Wire Filler Metal

Tlhaloso e Khutšoanyane:

ER-Ni1 e sebelisoa bakeng sa ho cheselletsa le ho koala li-alloys tsa Nickel 200 le Nickel 201.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

Nickel AlloyWelding WireTig WireERNi-1

Litekanyetso
EN ISO 18274 - Ni 2061 - NiTi3
AWS A5.14 – ER Ni-1

 

Likarolo le Lisebelisoa

ER-Ni1 e sebelisoa bakeng sa ho cheselletsa le ho koala li-alloys tsa Nickel 200 le Nickel 201.

E nepahetse bakeng sa ho kopanya li-alloys tsa Monel le koporo-nikeleli-alloys ho litšepe tsa carbon.

Ni1 e na le titanium e lekaneng ho laola porosity ea weld-metal lits'ebetsong tsa welding.

Ka tloaelo e sebelisoa indastering ea ts'ebetso ea lik'hemik'hale, tlhahiso ea fiber ea maiketsetso le lisebelisoa tsa ho lokisa lijo joalo-joalo.

 

Lisebelisoa tse Tloaelehileng tsa Base

Nickel 200 le 201*
* Lethathamo la litšoantšo, eseng le felletseng

 

Sebopeho sa Lik'hemik'hale %
C% Mn% Fe% P% S% Si%  
max max max max max max  
0.05 0.80 0.70 0.030 0.010 0.75  
             
Cu% Ni% Co% Ti% Al%    
max 93.00 max 2.00 max    
0.20 min 1.00 3.50 1.00    

 

Thepa ea Mechini
Matla a tšepe ≥410 MPa  
Kotulo Matla ≥200 MPa  
Elongation ≥30 %  
Matla a Tšusumetso ≥100 J  

Thepa ea mechine e hakanngoa 'me e ka fapana ho latela mocheso, khase e sireletsang, li-parameter tsa welding le lintlha tse ling.

 

Likhase Tsa Tšireletso

TS EN ISO 14175 TIG: I1 (Argon)

 

Maemo a Welding

TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Lintlha tsa ho paka
Diameter Bolelele Boima ba 'mele  
1.60 limilimithara

2,40 limilimithara

1000 limilimithara

1000 limilimithara

5 Kg

5 Kg

 

 