Terata ea ho Wellisa ea Nickel Alloy ea ERNiFeCr-1, Tšepe ea ho Tlatsa ea Nickel Tig

Tlhaloso e Khutšoanyane:

Alloy 825 (ERNiFeCr-1) ke terata ea nickel-iron-chromium e etsang hore ena e be khetho e loketseng bakeng sa mefuta e fapaneng ea lits'ebetso tse thata.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Motsoako oa nikeleTerata ea ho tjheseletsaTerata ea TigERNiFeCr-1

Maemo
EN ISO 18274 - Ni 8065 - NiFe30Cr21Mo3
AWS A5.14 – ER NiFeCr-1

 

Likarolo le Litšebeliso

Motsoako oa 825 kenikeli-terata ea tšepe-chromium e etsang hore ena e be khetho e loketseng bakeng sa mefuta e fapaneng ea lits'ebetso tse thata.

Terata ena e fana ka maemo a hodimo a ho hanyetsa mafome dibakeng tse etsang hore oxidize le tse fokotsang mafome ka tekanyo.

E loketse hantle bakeng sa ho koahela ka holimo moo ho hlokahalang metsoako e tšoanang ea lik'hemik'hale.

Ho tjheseletsa hantle haholo ka tshepe e tshepe e tshepehang ka botlalo e nang le kganyetso e phahameng kgahlanong le ho petsoha ha mafome a kgatello mecheng e nang le di-ion tsa chloride.

Hangata e sebelisoa indastering ea ts'ebetso ea lik'hemik'hale, petrochemical, tlhahiso ea pampiri le tlhahiso ea motlakase jj.

 

Lisebelisoa tse Tloaelehileng tsa Motheo

G-X7NiCrMoCuNb 25 20, X1NiCrMoCuN25 20 6, X1NiCrMoCuN25 20 5, NiCr21Mo, X1NiCrMoCu 31 27 4, N08926, N08904, ALLOY 825, N08028, UNS N08825 W.Nr: 1.4500, 1.4529, 1.4539 (904L), 2.4858, 1.4563, 1.4465, 1.4577 (310Mo), 1.4133, 1.4500, 1.4503, 1.4505, 1.4506, 1.4531, 1.4536, 1.4585, 1.4586*
* Lethathamo le hlalosang, eseng le felletseng

 

Sebopeho sa Lik'hemik'hale %

C%

Mn%

Fe%

P%

S%

Si%

 

boholo

0.70

22.00

boholo

boholo

boholo

 

0.05

0.90

motsotso

0.020

0.004

0.50

 

 

Cu%

Ni%

Al%

Ti%

Cr%

Mo%

 

2.30

43.00

boholo

1.00

22.00

3.00

 

3.00

46.00

0.20

1.20

23.50

3.50

 

 

Matlotlo a Mekaniki
Matla a tšepe ≥550 MPa  
Matla a Tekanyo -  
Ho lelefatsa -  
Matla a Tšusumetso -  

Thepa ea mechini ke ea khakanyo 'me e ka fapana ho latela mocheso, khase e sireletsang, liparamente tsa ho tjheseletsa le lintlha tse ling.

 

Likhase tse Sireletsang

TS EN ISO 14175 TIG: I1 (Argon)

 

Maemo a ho tjheseletsa

TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Lintlha tsa ho paka
Bophara Bolelele Boima ba 'mele  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 kg

5 kg

5 kg

 

 

Boikarabello: Le hoja ho entsoe boiteko bohle bo utloahalang ho netefatsa ho nepahala ha tlhahisoleseling e ka har'a eona, tlhahisoleseling ena e ka fetoha ntle le tsebiso 'me e ka nkoa e loketse feela bakeng sa tataiso e akaretsang.

 


  • E fetileng:
  • E 'ngoe: