ECoCr-A (Cobalt 6) Cobalt Hardfacing le Electrode ea ho Welding e sa Tshweng

Tlhaloso e Khutšoanyane:

Cobalt Hardfacing & Electrode ea ho Welding e sa Tloheng


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

ECoCr-A (Cobalt 6)Cobalt Hardfacing & Electrode ea ho Welding e sa Tloheng

Mofuta oa motsoako:A5.13, Li-electrode tsa ho tjheseletsa tse tiileng le liropo tsa ho tjheseletsa, A5.13

ECoCr-A Cobalt Alloy 6 ke eona e sebelisoang haholo ke li-alloy tse thehiloeng ho cobalt tse hanang ho robeha 'me e bontša ts'ebetso e ntle ka ho feletseng. E nkoa e le tekanyetso ea indasteri bakeng sa lits'ebetso tsa ho hanyetsa ho robeha ka kakaretso, e na le khanyetso e ntle ho mefuta e mengata ea ho senyeha ha mechine le lik'hemik'hale ho pholletsa le mocheso o pharaletseng, 'me e boloka boemo bo loketseng ba ho thatafala ho fihlela ho 500⁰C (930⁰F). E boetse e na le khanyetso e ntle khahlanong le tšusumetso le khoholeho ea cavitation. Cobalt Alloy 6 e loketse hantle mekhoa e fapaneng ea ho tiisa 'me e ka fetoloa ka lisebelisoa tsa carbide.

Sehlopha sa AWS: ECoCr-A Setifikeiti: AWS A5.13/A5.13M:2010
Motsoako: ECoCr-A ASME SFA A5.13
Boemo ba ho tjheseletsa: F, V, OH, H Hona joale:*NS
Matla a ho Tenyetseha, kpsi: *NS
Matla a Tlhahiso, kpsi: *NS
Ho lelefatsa %: *NS

Ditshebediso tse Tloaelehileng: di-blade tsa ho kuta; di-valve tsa phallo ya mokelikeli; di-screw tsa extrusion; di-bushing tsa roll; mocheso o phahameng; bokaholimo ba di-valve.

K'hemistri e Tloaelehileng ea Lithapo ho latela AWS A5.13 (boleng bo le bong ke bo phahameng ka ho fetisisa)

C Mn Si Cr C Fe W Co
0.7-1.4 ≤2.0 ≤2.0 25-32 0.7-1.4 ≤5.0 3.0-6.0 Bala