Tlhaloso e Khutšoanyane:

Electrode ea tšepe ea carbon e koahetsoeng ka phofo e tlase ea haedrojene-potasiamo-tšepe.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

AWS A5.1 E7028 Tjheseletsa Rods

Ho tjheseletsa AWS A5.1 E7028 ke electrode ya tshepe ya khabone e nang le haeterojene e tlase, potassium, tshepe, e nang le phofo e nyane. Phofo ya tshepe e ka hara seaparo e eketsa sekgahla sa ho tjheseletsa ho fihlela ho 180%. E na le tshebediso e ntle haholo e e nolofalletsang ho ba le arc e tsitsitseng, e nang le ho fafatsa ho tlase, ho tlosa slag ho bonolo mme e etsa ho tjheseletsa maemong ohle. Tshepe e tjheseditseng e na le thepa e ntle ya mechini e fanang ka ho tiea ho hotle haholo ha mocheso o tlase.

Kopo

AWS A5.1 E7028 e sebediswa ho welding ya fillet e bataletseng le e bataletseng meahong e entsweng ka tshepe ya khabone le tshepe e nang le alloy e tlase jwalo ka ditshepe tsa 16Mn, 09Mn2Si le A, B, D, E tse sebediswang ho aha dikepe.

Sebopeho sa Lik'hemik'hale (%)

Sebopeho sa Lik'hemik'hale

C

Mn

Si

S

P

Ni

Cr

Mo

V

Boleng ba Tiisetso

≤0.15

≤1.60

≤0.90

≤0.035

≤0.035

≤0.30

≤0.20

≤0.30

≤0.08

Sephetho se Akaretsang

0.077

1.03

0.35

0.005

0.014

0.011

0.028

0.007

0.016

 

Matlotlo a Mekaniki a Tšepe e Lahliloeng

Ntho ea Teko

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) -30°C

Boleng ba Tiisetso

≥490

≥400

≥20

≥27

Sephetho se Akaretsang

535

430

26

189

Referense ea Hona Joale (DC)

Bophara

φ4.0

φ5.0

Amperage

180 ~ 240

210 ~ 280

Lintlha:

1. Electrode e tlameha ho futhumatsoa mochesong oa 350°C ka hora e le 'ngoe. Chesa thupa neng kapa neng ha e sebelisoa.

2. Litšila tse kang mafome, matheba a oli le mongobo li lokela ho tlosoa mosebetsing.

3. Ho hlokahala seqha se sekgutshwane ho etsa tjheseletso. Tsela e moqotetsane ya tjheseletso e a kgethwa.

Polokelo le ho baka ha Electrode ea ho Welding ea E7028

Kaha e na le electrode e tlase ea haeterojene, E7016 e hlokaho baka/ho omisapele o sebedisa. Mocheso o kgothaletswang wa ho omisa kapa ho baka bakeng sa thupa ya E7028 ho ya ka AWS A5.1, Tafole ya 1.3 ke 500-800°F (260-425°C) ka dihora tse 1-2.

Electrode e besitsoeng kapa e omisitsoeng e lokela ho bolokoa ka ontong e nkehang habobebe mochesong oa 50-250°F (30-140°C) nakong ea tšebeliso. Electrode e sa sebelisoang e lokela ho khutlisetsoa liontong tse sa sisinyeheng.