Tlhaloso e Khutšoanyane:

L109 (AWS/ASME A 5.3 E 4043) ke electrode e hloekileng ea aluminium e nang le lera le thehiloeng letsoai. Sebelisa DCEP (electrode ea motlakase o tobileng e ntle). Leka ho sebelisa arc e khutšoanyane ho tjheseletsa.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Electrode ea Aluminium le Aluminium Alloy

L109                                                     

GB/T E1100

AWS A5.3 E1100

Tlhaloso: L109 ke electrode e hloekileng ea aluminium e nang le lera le thehiloeng letsoai. Sebelisa DCEP (electrode ea hona joale e tobileng e ntle). Leka ho sebelisa arc e khutšoanyane ho tjheseletsa.

Tšebeliso: E sebelisoa bakeng sa ho tjheseletsa lipoleiti tsa aluminium le lijana tsa aluminium tse hloekileng.

Sebopeho sa lik'hemik'hale sa tšepe e welded (%):

Si+Fe

Cu

Mn

Zn

Al

Tse ling

≤0.95

0.05 ~ 0.20

≤0.05

≤0.10

≥99.0

≤0.15

 

 

Litšobotsi tsa mechini tsa tšepe e welded:

Ntho ea teko

Matla a tšepe

Mpa

E tiiselitsoe

≥80

 

 

Khoeli e khothaletsoang:

Bophara ba molamu

(mm)

3.2

4.0

5.0

Hona joale ho tjheseletsa

(A)

80 ~ 100

110 ~ 150

150 ~ 200

 

Tsebiso:

1. Electrode e bonolo haholo ho angoa ke mongobo, kahoo e lokela ho bolokoa ka setshelong se omileng se sa keneng moya ho thibela hore e se ke ea senyeha ka lebaka la mongobo; electrode e tlameha ho besoa mochesong o ka bang 150°C lihora tse 1 ho isa ho tse 2 pele e tjheseletsa;

2. Lipoleiti tsa ho kenya li lokela ho sebelisoa pele ho tjheseletsa, 'me tjheseletsa e lokela ho etsoa ka mor'a ho futhumatsa pele ho 200 ~ 300°C ho latela botenya ba tjheseletsa; molamu oa tjheseletsa o lokela ho ba o otlolohileng holim'a bokaholimo ba tjheseletsa, arc e lokela ho ba khutšoanyane kamoo ho ka khonehang, 'me ho nkeloa sebaka ha lithupa tsa tjheseletsa ho lokela ho etsoa kapele;

3. Ho tjheseletsa ho lokela ho hlwekiswa oli le ditshila pele ho tjheseletsa, mme slag e lokela ho tloswa ka hloko kamora ho tjheseletsa, mme e hlatswe ka mouoane kapa metsi a chesang.

 

Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka selemo sa 2000. Re 'nile ra kopanela tlhahisong ea li-electrode tsa ho tjheseletsa, lithupa tsa ho tjheseletsa le lisebelisoa tse sebelisoang tsa ho tjheseletsa ka lilemo tse fetang 20.

Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa li-electrode tsa tšepe e sa hloekang, li-electrode tsa tšepe ea khabone, li-electrode tsa ho tjheseletsa tse nang le alloy e tlase, li-electrode tsa ho tjheseletsa tse holim'a metsi, li-electrode tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tse nang le alloy e bobebe le e nang le alloy e tlase, lithapo tsa ho tjheseletsa tse nang le alloy e sirelelitsoeng ke khase, lithapo tsa ho tjheseletsa tsa aluminium, ho tjheseletsa ka har'a arc e ka tlas'a metsi. lithapo, lithapo tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tsa koporo, lithapo tsa ho tjheseletsa tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tse sehang khabone, le lisebelisoa tse ling tsa ho tjheseletsa le tse sebelisoang.

 


  • E fetileng:
  • E 'ngoe: