AWS/ASME 5.3 E 4047 Aluminium Welding Electrodes Aluminium Welding Rods Arc Welding Stick Supplier

Tlhaloso e Khutšoanyane:

Bakeng sa aluminium ea arc welding e kopantsoeng le koporo, silicon, le magnesium


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

EN 573-3: E AlSi12

DIN 1732: EL-Al Si12

LIKETSAHALO LE LITSEBETSI:

Bakeng sa aluminium ea arc welding e kopantsoeng le koporo, silicon, le magnesium.

E boetse e ntle bakeng sa ho kopanya likarolo tse fapaneng tsa aluminium.

12% Silicon aluminium arc welding electrode e nang le slag e ikhethang ea ho iphahamisa.Limaraka tse ling tsa aluminium tse kang Al 99, Al Mn, joalo-joalo li fumaneha hape.

Slag e ikhethang ea ho ipholla.

Bophelo bo bosoeu bo bosoeu bo bolelele ba nako e telele bo tlokomang bo tlokoma lihlahisoa tse tloaelehileng ho hanyetsa mongobo.
E ka etsoa ka mebala e fapaneng e tloaelehileng.

E fumaneha ka har'a makotikoti a PURE ALUMINIUM a koetsoeng ka hermetically kapa mekotla ea foil e pakiloeng bakeng sa nako e telele.

E fumaneha hape ka foromo ea TIG joalo ka khoutu ea lintlha 6047, ka foromo ea MIG e le khoutu ea 7091 hape e le feela.

Alloy ea ho KHANYA TSELA JOALOKAHA KHOUTU EA 2191:

All Weld Metal Analysis (Tsela e Tloaelehileng Boima %)
'Mala oa Flux: Mebala e Mosoeu kapa e Tloaelehileng
12.1 .001 .15 .01 .003 .001
Si Cu Fe Mg Mn Zn
Welding Current & Litaelo
E khothalelitsoeng Hajoale: DC Reverse (+)
Diameter (mm) 3/32 (2.5) 1/8 (3.25)
Bonyane Amperage 50 70
Maximum Amperage 80 120

Mekhoa ea ho Welding: Qala ka ho sebelisa karolo e ka holimo ea mefuta ea amperage.Fepa electrode ka potlako 'me u tsamaee ka potlako ho boloka lekhalo le haufi haholo la arc.
Maemo a ho cheselletsa: a bataletseng, a tšekaletseng

DEPOSITION REATES:

Diameter(mm) Bolelele(mm) Weldmetal/Elektrode Electrodes ka lb (kg) ea Weldmetal Nako ea ho beha Arc min/lb (kg) Litlhophiso tsa Amperage RecoveryRate
3/32 (2.5) 14″(350) .14oz (4.3g) 114 (251) 110 (242) 70 90%
1/8 (3.25) 14″ (350) .23oz (6.5g) 70 (153) 62 (136) 110 90%
5/32 (4.0) 14″ (350) .33oz (9.6g) 48 (107) 47 (103) 135 90%

KAKARETSO YA HO PAKAJWA ELECTRODE LE MEKMO:

3/32 (2.5) 1/8 (3.25)
Bolelele (mm) 14″ (350) 14″ (350)
Li-electrode / lb 49 33
Li-electrode / lik'hilograma 108 73