AWS EN-C1 (Z308) Nickel e Pure Cast Iron Welding Electrode Nickel 99 Welding Rods Arc Stick Electrodes Ni99

Tlhaloso e Khutšoanyane:

AWS ENi-C1 (Z308) ke electrode ea tšepe e entsoeng ka tšepe e nang le tšepe e tlaase ea carbon le coat e matla ea graphitized.


Lintlha tsa Sehlahisoa

Li-tag tsa Sehlahisoa

Lahlela Iron Welding Electrode

Z308                                                     

GB/T EZNi-1

AWS A5.15 EN-C1

Tlhaloso: Z208 ke electrode ea tšepe e entsoeng ka tšepe e nang le mokokotlo o tlaase oa carbon steel le seaparo se matla sa graphitized.E ka sebelisoa bakeng sa AC le DC ka bobeli.The weld e ka fetoha tšepe e 'mala o moputsoa ha e pholile butle, empa ho hanyetsa ha eona crack ho fokola.

Kopo: E sebelisetsoa ho lokisa mefokolo ea tšepe e bohlooho.

 

Sebopeho sa lik'hemik'hale tsa tšepe ea weld(%):

C

Si

Mn

S

Ni

Fe

Ba bang

≤2.0

≤2.5

≤1.0

≤0.03

≥90

≤8.0

≤1.0

 

Nako e khothalelitsoeng:

Bophara ba molamu

(mm)

2.5

3.2

4.0

Hona joale welding

(A)

Lilemo tse 65-90

90 ~ 110

120 ~ 150

 

Tlhokomeliso:

1. Electrode e tlameha ho behoa bakeng sa hora e le 1 ho pota 150 ℃ pele ho ts'ebetso ea welding;

2. Khatello ea maikutlo sebakeng sa ho lokisa welding e ka felisoa ka ho phunya weld ho qoba mapetsong.

 

 

Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka selemo sa 2000. Re qetile lilemo tse fetang 20 re etsa li-electrode tsa welding, lithupa le lisebelisoa tsa ho cheselletsa.

Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa li-electrode tsa tšepe tse sa hloekang, li-electrode tsa tšepe tsa carbon, li-electrode tse tlase tsa welding, li-electrode tsa welding, nickel & cobalt alloy welding wires, tšepe e bonolo le lithapo tse tlase tsa alloy, lithapo tsa tšepe tse se nang tšepe, likhoele tse sirelelitsoeng ka khase, lithapo tsa aluminium tse cheselletsang, li-arc tse kentsoeng ka metsing.lithapo, lithapo tsa nickel & cobalt alloy welding, lithapo tsa tšepe tsa koporo, lithapo tsa welding tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tsa carbon gouging, le lisebelisoa tse ling tsa welding & consumables.

 