Lithupa tsa ho Wellisa tsa Tšepe e sa Khaotseng tsa AWS E309L-15, Sehokelo sa Tšepe e sa Khaotseng sa Arc Wellisa Electrode

Tlhaloso e Khutšoanyane:

A067 (AWS E309L-15) ke electrode ea tšepe e sa hloekang ea mofuta oa sodium e nang le haeterojene e tlase haholo ea Cr23Ni13.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Ho tjheseletsa Tšepe e sa KhaotsengElektrode

A067                                         

GB/T E309L-15

AWS E309L-15

Tlhaloso: A067 ke electrode ea tšepe e sa hloekang ea mofuta oa sodium e nang le hydrogen e tlase haholo ea Cr23Ni13. Sebelisa DCEP (electrode ea hona joale e tobileng) 'me e ka kopanngoa libakeng tsohle. E na le khabone e tlase, kahoo e ka hanela ho bola ha li-intergranular ho bakoang ke pula ea carbide ntle le li-stabilizer tse kang niobium le titanium.

Tšebeliso: E sebelisoa bakeng sa mofuta o tšoanang oa sebopeho sa tšepe e sa ruseng, tšepe e kopantsoeng le likarolo tsa tšepe tse bōpehileng joaloka tse khethehileng tlhahisong ea faeba ea maiketsetso, petrochemical le lisebelisoa tse ling. E ka boela ea sebelisoa bakeng sa ho koahela mekhahlelo ea phetoho leboteng le ka hare la likepe tsa khatello ea reactor ea nyutlelie le ho tjheseletsa likarolo tsa ka hare tsa tora.

 

Sebopeho sa lik'hemik'hale sa tšepe e welded (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Litšobotsi tsa mechini tsa tšepe e welded:

Ntho ea teko

Matla a tšepe

Mpa

Ho lelefatsa

%

E tiiselitsoe

≥520

≥25

 

Khoeli e khothaletsoang:

Bophara ba molamu

(mm)

2.5

3.2

4.0

5.0

ho tjheseletsa hona joale

(A)

50 ~ 70

80 ~ 120

130 ~ 160

160 ~ 200

 

Tsebiso:

1. Electrode e lokela ho besoa hora e le 'ngoe mochesong o ka bang 300℃ pele ho ts'ebetso ea ho tjheseletsa;

2. Ho bohlokoa ho hlwekisa mafome, sekala sa oli, metsi le litšila likarolong tsa ho tjheseletsa pele ho tjheseletsa.

 

Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka selemo sa 2000. Re ntse re etsa tlhahiso eaelektrode ea ho tjheseletsas, lithupa tsa ho tjheseletsalelintho tse sebelisoang ho tjheseletsaka lilemo tse fetang 20.

Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa li-electrode tsa tšepe e sa hloekang, li-electrode tsa tšepe ea khabone, li-electrode tsa ho tjheseletsa tse nang le alloy e tlase, li-electrode tsa ho tjheseletsa tse holim'a metsi, li-electrode tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tse nang le alloy e bobebe le e nang le alloy e tlase, lithapo tsa ho tjheseletsa tse nang le alloy e sirelelitsoeng ke khase, lithapo tsa ho tjheseletsa tsa aluminium, ho tjheseletsa ka har'a arc e ka tlas'a metsi. lithapo, lithapo tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tsa koporo, lithapo tsa ho tjheseletsa tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tse sehang khabone, le lisebelisoa tse ling tsa ho tjheseletsa le tse sebelisoang.


  • E fetileng:
  • E 'ngoe: