Terata ea ho tjheseletsa ea motsoako oa nikeli ERNiCr-3 Nickel Tig Wire Filler Metal

Tlhaloso e Khutšoanyane:

Motsoako oa 82 (ERNiCr-3) o sebelisetsoa ho tjheseletsa metsoako ea 600, 601, 690, 800 le 800HT jj.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Motsoako oa nikeleTerata ea ho tjheseletsaTerata ea TigERNiCr-3

Maemo
EN ISO 18274 - Ni 6082 - NiCr20Mn3Nb
AWS A5.14 – ER NiCr-3

 

Likarolo le Litšebeliso

Motsoako oa 82 o sebelisetsoa ho tjheseletsa li-alloy tse 600, 601, 690, 800 le 800HT jj.

Tšepe e welletsoeng e na le matla a phahameng le khanyetso e ntle ea mafome, ho kenyeletsoa le khanyetso ea oxidation le matla a ho phatloha ha ho thekesela mochesong o phahameng.

E loketse lits'ebetso tse fapaneng tsa ho tjheseletsa lipakeng tsa mefuta e fapaneng eanikelilitšepe tse kopantsoeng, litšepe tse sa ruseng, litšepe tsa khabone ho kenyeletsoa le tse koahetsoeng.

E loketse lits'ebetso tse fapaneng ho tloha ho cryogenic ho isa mochesong o phahameng, e leng se etsang hore motsoako ona e be o mong oa e sebelisoang haholo lelapeng la nickel.

Hangata e sebelisoa indastering ea tlhahiso ea motlakase le ea petrochemical jj.

Lisebelisoa tse Tloaelehileng tsa Motheo

Motsoako oa 600, Motsoako oa 601, Motsoako oa 690, Motsoako oa 800, Motsoako oa 330*
* Lethathamo le hlalosang, eseng le felletseng

 

 

Sebopeho sa Lik'hemik'hale %

C%

Mn%

Fe%

P%

S%

Si%

 

boholo

2.50

boholo

boholo

boholo

boholo

 

0.05

3.50

3.00

0.030

0.015

0.50

 

 

Cu%

Ni%

Co%

Ti%

Cr%

Nb+Ta%

 

boholo

67.00

boholo

boholo

18.00

2.00

 

0.50

motsotso

1.00

0.75

22.00

3.00

 

 

Matlotlo a Mekaniki
Matla a tšepe ≥600 MPa  
Matla a Tekanyo ≥360 MPa  
Ho lelefatsa ≥30 MPa  
Matla a Tšusumetso ≥100 MPa  

Thepa ea mechini ke ea khakanyo 'me e ka fapana ho latela mocheso, khase e sireletsang, liparamente tsa ho tjheseletsa le lintlha tse ling.

 

Likhase tse Sireletsang

TS EN ISO 14175 TIG: I1 (Argon)

 

Maemo a ho tjheseletsa

TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Lintlha tsa ho paka
Bophara Bolelele Boima ba 'mele  
1.60 mm

2.40 mm

1000 mm

1000 mm

5 kg

5 kg

 

 