Liropo tsa ho Welda tsa Tšepe ea Khabone ea ER70S-2, Litšepe tse Tlatsang bakeng sa Terata ea ho Welda e Sirelelitsoeng ke Khase, Mofani ea Molemohali oa ho Solder

Tlhaloso e Khutšoanyane:

ER70S2 ke terata ea boleng bo holimo ea MIG le TiG bakeng sa ho tjheseletsa mefuteng eohle ea litšepe tse bobebe le tsa khabone, e hlahisang li-weld tsa boleng bo holimo tse nang le masoba a fokolang.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

ER70S2 ke terata ea boleng bo holimo ea MIG & TiG bakeng sa ho tjheseletsa mefuteng eohle ea litšepe tse bobebe le tsa khabone, e hlahisang li-weld tsa boleng bo holimo tse nang le masoba a fokolang. Ke terata e nang le deoxidized triple (Zirconium, Titanium, le Aluminium) e etsang hore e be khetho e ntle bakeng sa ho tjheseletsa holim'a mafome le sekala sa sile. Ha ho hlokahale flux ka sehlahisoa sena.

LITLHAKISO TSE TLWAELEHILENG:

liphaephe le mechine ea ho cheka ea lebōpong la leoatle, mosebetsi oa tšepe ea meaho

Boemo ba ho tjheseletsa: F, V, OH, H Hona joale: DCEP
Matla a ho Tenyetseha, kpsi: 70
Matla a Tlhahiso, kpsi: 58
Ho lelefatsa ka 2”%: 22

Charpy V-Notch e Tloaelehileng: 35 ft.-lb. Ho -20 deg F

K'hemistri e Tloaelehileng ea Lithapo ho latela AWS A5.18 (boleng bo le bong ke bo phahameng ka ho fetisisa)

C Mn Si P S Ni Cr Mo V Cu Ti Zr Al
0.07 0.90-1.40 0.40-0.70 0.025 0.035 0.15 0.15 0.15 0.03 0.50 0.05-0.15 0.02-0.12 0.05-0.15
Liparamitha tse Tloaelehileng tsa ho Welding
Bophara Tshebetso Volt Li-amplifier Khase e Sireletsang
in (mm)
.035 (0.9) GMAW 28-32 165-200 Phetiso ea Spray 98% Argon+2% Oksijene kapa 75% Argon+25% CO2
.045 (1.2) GMAW 30-34 180-220 Phetiso ea Spray 98% Argon+2% Oksijene kapa 75% Argon+25% CO2
1/16 (1.6) GMAW 30-34 230-260 Phetiso ea Spray 98% Argon+2% Oksijene kapa 75% Argon+25% CO2
.035 (0.9) GMAW 22-25 100-140 Phetisetso e Khutšoanyane ea Potoloho 100% CO2 kapa 75% Argon +25% CO2
.045 (1.14) GMAW 23-26 120-150 Phetisetso e Khutšoanyane ea Potoloho 100% CO2 kapa 75% Argon +25% CO
1/16 (1.6) GMAW 23-26 160-200 Phetisetso e Khutšoanyane ea Potoloho 100% CO2 kapa 75% Argon +25% CO
.035 (0.9) GTAW 13-16 60-100 Argon ea 100%
.045 (1.14) GTAW 13-16 70-120 Argon ea 100%
1/16 (1.6) GTAW 12-15 100-125 Argon ea 100%
3/32 (2.4) GTAW 15-20 125-175 Argon ea 100%
1/8 (3.2) GTAW 15-20 175-250 Argon ea 100%