A5.13 ECoCr-C Cobalt Alloy Hardfacing Welding Rods Hardfacing Welding Electrode Arc Welding Stick

Tlhaloso e Khutšoanyane:

Liropo tsa ho Welding tsa A5.13 ECoCr-C Cobalt Alloy Hardfacing e sebelisetsoa lihlooho tsa li-valve tsa ho welding, masale a tiiso a pompo ea khatello e phahameng le likarolo tsa li-crusher.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

 

Tlhaloso ea AWS:AWS A5.13/AME A5.13 ECoCr-C
LIKOPELO:

Bokaholimo bo thata ba lihlooho tsa li-valve, masale a tiiso a pompo ea khatello e phahameng le likarolo tsa li-crusher.
TLHALOSO:

Electrode e koahetsoeng ke COBALTARD 1FC ke motsoako o tloaelehileng oa ho thatafala o phahameng ka ho fetisisa sehlopheng sa metsoako ea cobalt e sebelisetsoang ho robeha ha mocheso o phahameng o amanang le ho robeha. Li-deposit tsa motsoako ona li na le bongata bo boholo ba lik'habohaedreite tsa chromium tse amang khanyetso e ikhethang ea ho robeha ha mocheso. Ho eketsoa ha tungsten ho eketsa ho thatafala ha mocheso o phahameng le ho tiea ha matrix bakeng sa sekhomaretsi se setle le khanyetso e tiileng ea ho robeha ha likaroloana. E hokahana hantle le litšepe tsohle, ho kenyeletsoa le tse sa hloekang.
LINTLHA TSA TŠEBELISO:

Futhumatsa ho 300ºC ho ea holimo ka kakaretso. Sebelisa lithupa tse bontšang mocheso oa PHILARC kapa sesupa-tsela sa mocheso oa PHILARC ho fumana hore na mocheso o nepahetseng o finyelloa pele ho tjheseletsa. Bakeng sa lintlha tse ling sheba Chate ea PHILARC 4 Mehato e Bonolo ea ho tjheseletsa.

Ho sebetsa hantle ho futhumatsa mochesong oa 600ºC le ho pholisa butle ka mor'a ho tjheseletsa ho thibela ho petsoha.

Omisa di-electrode ho 150-200ºC metsotso e 30 - 60 pele o di sebedisa. Sebedisa dionto tsa ho omisa tse nkehang habobebe tsa PHILARC.

BOTHATA BA SHEBELLO EA TŠEPE EA HO WELDA: 50 – 56 HRC (520- 620 Hv)
Sebopeho sa lik'hemik'hale se Tloaelehileng sa Tšepe ea Weld (%):

C Si Mn Cr W Co
2.15 0.47 1.03 31.25 12.72 Bala

BOHOLO BO FUMANEHANG LE BO KHOTHALETSOANG (DC +):

Boholo (bophara ba mm) 3.2 4.0 5.0
Bolelele (mm) 350 350 350
Mefuta ea Hona Joale (Amp) 90 - 120 110 - 150 140 - 180

 

 