ECoCr-B Cobalt Alloy 12 Hardfacing Welding Rods Electrode Arc Welding Stick e hanelang ho roala

Tlhaloso e Khutšoanyane:

Mofuta oa motsoako: A5.13, Li-electrode tsa ho tjheseletsa tse tiileng le liropo tsa ho tjheseletsa, A5.13


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

ECoCr-B (Cobalt 12) Cobalt Hardfacing le Electrode ea ho Welding e sa Tshweng

Mofuta oa motsoako: A5.13, Li-electrode tsa ho tjheseletsa tse tiileng le liropo tsa ho tjheseletsa, A5.13
ECoCr-B Cobalt Alloy 12 e ka nkoa e le motsoako o mahareng pakeng tsa Cobalt Alloy 6 le Cobalt Alloy 1. E na le karolo e phahameng ea li-carbide tse thata, tse robehang habonolo ho feta Cobalt Alloy 6, 'me e na le khanyetso e eketsehileng khahlanong le khoholeho ea angle e tlase, ho hohlana, le ho senyeha ho matla ha e ntse e boloka tšusumetso e utloahalang le khanyetso ea cavitation. Cobalt Alloy 12 hangata e sebelisoa e ikemetse kapa e sebetsa khahlanong le Cobalt Alloy 6 kapa 1. Boleng bo phahameng ba tungsten bo fana ka thepa e betere ea mocheso o phahameng ha e bapisoa le Cobalt Alloy 6, 'me e ka sebelisoa mochesong o fihlang ho 700⁰C. Cobalt Alloy 12 hangata e sebelisoa bakeng sa lisebelisoa tsa ho seha tse hlokang ho mamella ho hohlana, mocheso le mafome.

Litšebeliso tse Tloaelehileng: mekoallo ea sakha ea ketane; meno a sakha; li-dies tsa extrusion

Sehlopha sa AWS: ECoCr-B Setifikeiti: AWS A5.13/A5.13M:2010
Motsoako: ECoCr-B ASME SFA A5.13

 

Boemo ba ho tjheseletsa:
F, V, OH, H
Hona jwale:
*NS

 

Matla a ho Tenyetseha, kpsi: *NS
Matla a Tlhahiso, kpsi: *NS
Ho lelefatsa %: *NS

*NS Ha ea totobatsoa

K'hemistri e Tloaelehileng ea Lithapo ho latela AWS A5.13 (boleng bo le bong ke bo phahameng ka ho fetisisa)

C Mn Si Cr Ni Mo Fe W Co Tse ling
1.0-1.7 2.0 2.0 25-32 3.0 1.0 5.0 7.0-9.5 Khutlo 1.0

 