E71T-GS ke electrode e nang le tšepe ea khabone, e nang le flux cored bakeng sa tšebeliso ntle le khase e sireletsang kantle. Electrode ena e etselitsoe ho tjheseletsa tšepe ea khabone e nang le gauge e tšesaane, ho tloha ho 3/16” ho isa ho 22 gauge.
Ditshebediso tse Tloaelehileng: di-weldment tse fetang ka lekgetlo le le leng; sehlahiswa sena se etseditswe ho tjheseletsa ka katleho hodima thepa e tjheseditsweng ka lejwe mme se ka sebediswa le hodima dibaka tse itseng tse nang le aluminiyamu. E71T-GS ha e hloke tšireletso ya kgase ya kantle mme e lokela ho tjheseletsa ka DCEN (polarity e otlolohileng).
| Sehlopha sa AWS: E71T-GS | Setifikeiti: AWS A5.20/A5.20M:2005 |
| Motsoako: E71T-GS | AWS/ASME SFA A5.20 |
| Boemo ba ho tjheseletsa: H, F, V, O | Hona jwale: DCEN Polarity e otlolohileng |
| Matla a Tensile a Fetohang, kpsi: | 86.4min (Ho robeha ha tšepe ea motheo) |
| Teko ea Kobeho e Tataisoang | E fihlela litlhoko tsa AWS |
| Liparamitha tse Tloaelehileng tsa Terata | |||||
| Bophara | Tshebetso | Li-amplifier | Li-volt | Lebelo la Phepelo ea Terata | |
| in | (mm) | ||||
| .030″ | 0.8 | FCAW | 50 | 15 | 80 |
| FCAW | 100 | 16 | 225 | ||
| FCAW | 150 | 17 | 375 | ||
| FCAW | 175 | 17 | 445 | ||
| .035″ | 0.9 | FCAW | 75 | 15 | 70 |
| FCAW | 100 | 16 | 110 | ||
| FCAW | 150 | 17 | 180 | ||
| FCAW | 200 | 18 | 305 | ||
| .045″ | 1.2 | FCAW | 100 | 15 | 70 |
| FCAW | 150 | 16 | 120 | ||
| FCAW | 200 | 17 | 195 | ||
| FCAW | 225 | 17 | 245 | ||
| 1/6″ | 1.6 | FCAW | 150 | 17 | 60 |
| FCAW | 200 | 18 | 85 | ||
| FCAW | 250 | 18 | 135 | ||
| FCAW | 300 | 19 | 180 | ||
| 5/64” | .078 | FCAW | 200 | 19 | 60 |
| FCAW | 250 | 20 | 80 | ||
| FCAW | 300 | 21 | 115 | ||
| FCAW | 325 | 120 | 6.6 | ||
*Liparamente tsena li ka sebelisoa maemong 'ohle. Bokhoni ba ho tjheseletsa kantle ho boemo maemong a holimo a motlakase bo tla itšetleha ka botenya ba poleiti le tsebo ea ho tjheseletsa.
Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka selemo sa 2000. Re ntse re etsa li-electrode tsa ho tjheseletsa,lithupa tsa ho tjheseletsa, le lintho tse sebelisoang ho tjheseletsa ka lilemo tse fetang 20.
Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa li-electrode tsa tšepe e sa hloekang, li-electrode tsa tšepe ea khabone, li-electrode tsa ho tjheseletsa tse nang le alloy e tlase, li-electrode tsa ho tjheseletsa tse holim'a metsi, li-electrode tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tse nang le alloy e bobebe le e nang le alloy e tlase, lithapo tsa ho tjheseletsa tse nang le alloy e sirelelitsoeng ke khase, lithapo tsa ho tjheseletsa tsa aluminium, ho tjheseletsa ka har'a arc e ka tlas'a metsi. lithapo, lithapo tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tsa koporo, lithapo tsa ho tjheseletsa tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tse sehang khabone, le lisebelisoa tse ling tsa ho tjheseletsa le tse sebelisoang.