Terata ea ho tjheseletsa ea tšepe e sa hloekang ea E2209T1-1/T1-4

Tlhaloso e Khutšoanyane:

E ntlafalitsoe bakeng sa ho tjheseletsa ka maemo, ka bobeli e otlolohileng ho ea holimo le bakeng sa liphaephe tse tsitsitseng tse tšoanelehang maemong a ho tjheseletsa a ASME 5G kapa 6G (phaephe hangata e bophara ba > 150mm, lebota la > 15mm).
Boreleli ba ho weldability maemong ohle


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Sehlopha sa AWS E2209T1-1/T1-4Terata ea Ts'ebetso ea Core

LIKAROLOANA
E ntlafalitsoe bakeng sa ho tjheseletsa ka maemo, ka bobeli e otlolohileng ho ea holimo le bakeng sa mosebetsi oa liphaephe tse tsitsitseng tse tšoanelehang maemong a ho tjheseletsa a ASME 5G kapa 6G (hangata phaephe e bophara ba > 150mm, lebota la > 15mm).
Boreleli ba ho weldability maemong ohle
Ho tlosoa ha litšila ho babatsehang

Khase e Sireletsang
80% Argon / 20% CO2
100% CO2

Likarolo tsa Bohlokoa
• Boreleli ba ho tjheseletsa maemong ohle
• Sephutheloana se koetsoeng ka vacuum
• Ho tlosa mafome hantle haholo
• Setifikeiti se bontshang sebopeho sa depositi, nomoro ya ferrite, le thepa ya charpy impact e lekilweng @ -196°C (-320°F)

Sehlopha sa AWS E2209T1-1/T1-4Terata ea Ts'ebetso ea CoreSebopeho sa Lik'hemik'hale

C Cr Ni Mo Mn Si P S N Cu
.03 22.5 9.7 3.25 0.95 .60 0.03 .015 0.14 0.20
Thepa ea Mechanical ea Flux Core Wire ea Sehlopha sa AWS E2209T1-1/T1-4
Matla a tšepe 120,000 psi
Matla a Tekanyo 95,000 psi
Ho lelefatsa (%) 26%
Liparamitha tsa terata ea AWS Class E2209T1-1/T1-4 Flux Core
Bophara WFS (ipm) Amperage Li-volt ESO (ka hare) Sekhahla sa ho ntsha tjhelete
(liponto/hora)
.045” 250 130 22 5/8-3/4” 5.4
300 160 24 5/8-3/4” 6.3
425 200 26 5/8-3/4” 9.2
780 270 32 5/8-3/4” 16.2
1/16” 150 170 23 3/4-1” 5.4
195 215 25 3/4-1” 7.0
240 250 26 3/4-1” 8.6
320 305 27 3/4-1” 11.5

 

Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka selemo sa 2000. Re ntse re etsa li-electrode tsa ho tjheseletsa,lithupa tsa ho tjheseletsa, le lintho tse sebelisoang ho tjheseletsa ka lilemo tse fetang 20.

Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa li-electrode tsa tšepe e sa hloekang, li-electrode tsa tšepe ea khabone, li-electrode tsa ho tjheseletsa tse nang le alloy e tlase, li-electrode tsa ho tjheseletsa tse holim'a metsi, li-electrode tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tse nang le alloy e bobebe le e nang le alloy e tlase, lithapo tsa ho tjheseletsa tse nang le alloy e sirelelitsoeng ke khase, lithapo tsa ho tjheseletsa tsa aluminium, ho tjheseletsa ka har'a arc e ka tlas'a metsi. lithapo, lithapo tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tsa koporo, lithapo tsa ho tjheseletsa tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tse sehang khabone, le lisebelisoa tse ling tsa ho tjheseletsa le tse sebelisoang.


  • E fetileng:
  • E 'ngoe: