AWS: Terata e nang le di-Flux-core (FCAW-G) ya E81T1-Ni1C-JH4, E81T1-C1A4-Ni1-H4e etselitsoe lits'ebetso tse matla haholo, tse se nang motsoako o mongata tse sebelisang khase e sireletsang ea CO2 ea 100%.
Likaroloana
E khona ho hlahisa li-weld depositi tse nang le matla a ho thula a fetang 88 – 123 J (65 – 91 ft·lbf) ho -40°C (-40°F)
E etselitsoe ho tjheseletsa ka khase e sireletsang ea CO2 ea 100%
Tshebetso ea arc ea boleng bo holimo le ponahalo ea lifaha
E fihlela litlhoko tsa ho tela sebaka sa litšisinyeho tsa lefatše sa AWS D1.8
sephutheloana sa mokotla oa foil
| LITŠOANTŠISO | TLHAHISO | TLHOPHISO |
| AWS | AWS A5.29 | E81T1-Ni1C-JH4 |
| AWS | AWS A5.36 | E81T1-C1 A4-Ni1-H4 |
| ABS | ABS- Karolo ea 2 | 4YQ460SA H5 |
| CWB | CSA W48 | E551T1-C1A4-Ni1-H4 (E551T1-Ni1C-JH4) |
| DNV-GL | DNV-2.9 IV | Y46MS H5 |
| LR | LR – Khaolo ea 11 | 4Y46S H5 |
MOKHATLO OA DEPOSITO
| Tlhophiso | Khase e Sireletsang | Polarity | %B | %C | %Cr | %Mn | %Khoeli | %Ni | %P | %S | %SI | %V | Haedrojene e qhalanang Tšepe ea ho Weld ea mL/100g |
| E81T1-Ni1C-JH4 | 100% CO2 | DC+ | 0.12 max. | 0.15 max. | 1.5 e phahameng ka ho fetisisa. | 0.35 max. | 0.8-1.1 | 0.03 max. | 0.03 max. | 0.8 e phahameng ka ho fetisisa. | 0.05 max. | 4.0 max. | |
| E81T1-C1A4-Ni1-H4 | 100% CO2 | DC+ | 0.12 max. | 0.15 max. | 1.75 max. | 0.35 max. | 0.8-1.1 | 0.03 max. | 0.03 max. | 0.8 e phahameng ka ho fetisisa. | 0.05 max. | 4 e phahameng ka ho fetisisa. | |
| Sephetho se Tloaelehileng, Joalokaha se tjhesellelitsoe | 100% CO2 | DC+ | 0.0050-0.006 | 0.04-0.05 | 0.04-0.06 | 1.12-1.42 | 0.01 | 0.81-1 | 0.012 max. | 0.01 max. | 0.24-0.35 | 0.02- 0.03 | 1.7-3.2 |
LINTLHA
Ho hakanya ESO, tlosa 1/4 in. (6.0 mm) ho CTWD.
TLHOKOMELISO 1: Lintlha tsa teko ea tlatsetso ea tšepe ea sebopeho sa FEMA le AWS D1.8 li ka fumanoa sehlahisoa sena ho www.lincolnelectric.com.
TLHOKOMELISO 2: Sehlahisoa sena se na le likarolo tse kopanyang tse nyenyane. Tlhahisoleseling e eketsehileng e fumaneha ha e kopuoa.
Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka selemo sa 2000. Re ntse re etsa li-electrode tsa ho tjheseletsa,lithupa tsa ho tjheseletsa, le lintho tse sebelisoang ho tjheseletsa ka lilemo tse fetang 20.
Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa li-electrode tsa tšepe e sa hloekang, li-electrode tsa tšepe ea khabone, li-electrode tsa ho tjheseletsa tse nang le alloy e tlase, li-electrode tsa ho tjheseletsa tse holim'a metsi, li-electrode tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tse nang le alloy e bobebe le e nang le alloy e tlase, lithapo tsa ho tjheseletsa tse nang le alloy e sirelelitsoeng ke khase, lithapo tsa ho tjheseletsa tsa aluminium, ho tjheseletsa ka har'a arc e ka tlas'a metsi. lithapo, lithapo tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tsa koporo, lithapo tsa ho tjheseletsa tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tse sehang khabone, le lisebelisoa tse ling tsa ho tjheseletsa le tse sebelisoang.