AWS: E70T-6-H16, E70T6-A2-CS3-H16
AWS: Terata e sirelelitsoeng ka bo eona ea E70T-6-H16, E70T6-A2-CS3-H16 (FCAW-S) e nang le tšireletseho ea Flux-core. E etselitsoe ho tjheseletsa ka har'a sebaka, e nang le depositi e ngata holim'a tšepe ea carbon. E khothaletsoa ho tjheseletsa ka pass e le 'ngoe kapa tse ngata, ea othomathiki le ea semiautomatic.
LIKAROLOANA
Sekhahla se phahameng sa ho boloka thepa maemong a bataletseng le a bataletseng
Sekoti se boreleli le maemo a tlase a ho fafatsa
E khona ho hlahisa li-weld depositi tse nang le thepa ea tšusumetso e fetang 27 J (20 f:Ibf) ho -29°C (-20°F)
Li tjheseletsa poleiting e rusitseng hanyane kapa e se nang pula
Likopo tse Tloaelehileng
Tlhahiso ea poleiti e akaretsang
Tlhahiso ea meaho, ho kenyeletsoa le tse tlas'a litlhoko tsa ho sisinyeha ha lefatše
Libaka tsa likepe, ho tjheseletsa likepe tse thata ka likepeng
Marokho le lirifi tsa likepe tse lebōpong la leoatle
Li-weld tsa ho tjheseletsa holim'a li-tack tse entsoeng ka electrode ea thupa
MOKHATLO OA DEPOSITO
| Tlhophiso | Polarity | %Ai | %B | %C | %Mn | %P | %S | %SI | Haedrojene e qhalanang |
| Tšepe ea ho Weld ea mL/100g | |||||||||
| E70T-6- H8 | DC+ | 0.03 max. | 1.75 max. | 0.03 max. | 0.03 max. | 0.6 e phahameng ka ho fetisisa. | 8.0 e phahameng ka ho fetisisa. | ||
| E70T6- A2-CS3-H8 | DC+ | 0.03 max. | 1.75 max. | 0.03 max. | 0.03 max. | 0.6 e phahameng ka ho fetisisa. | 8 e phahameng ka ho fetisisa. | ||
| Sephetho se Tloaelehileng | DC+ | 0.7-1.0 | 0.0019 | 0.05-0.08 | 1.19-1.61 | 0.02 | 0.01 | 0.17-0.28 | 5.1 |
Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka selemo sa 2000. Re ntse re etsa li-electrode tsa ho tjheseletsa,lithupa tsa ho tjheseletsa, le lintho tse sebelisoang ho tjheseletsa ka lilemo tse fetang 20.
Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa li-electrode tsa tšepe e sa hloekang, li-electrode tsa tšepe ea khabone, li-electrode tsa ho tjheseletsa tse nang le alloy e tlase, li-electrode tsa ho tjheseletsa tse holim'a metsi, li-electrode tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tse nang le alloy e bobebe le e nang le alloy e tlase, lithapo tsa ho tjheseletsa tse nang le alloy e sirelelitsoeng ke khase, lithapo tsa ho tjheseletsa tsa aluminium, ho tjheseletsa ka har'a arc e ka tlas'a metsi. lithapo, lithapo tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tsa koporo, lithapo tsa ho tjheseletsa tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tse sehang khabone, le lisebelisoa tse ling tsa ho tjheseletsa le tse sebelisoang.