Liropo tsa ho Welding tsa AWS E7018 J506Fe Phofo ea Tšepe Electrode e Tlase ea Hydrogen Potassium

Tlhaloso e Khutšoanyane:

J506Fe (AWS E7018) ke electrode ea potassium e nang le phofo ea tšepe e nang le haeterojene e tlase. E sebelisoa ho AC le DC maemong 'ohle.


Qaqiso ea Sehlahisoa

Li-tag tsa Sehlahisoa

Electrode ea ho tjheseletsa ea Tšepe ea Khabone

J506Fe                                                  

GB/T E5018

AWS A5.1 E7018

Tlhaloso: J506Fe ke electrode ea potassium e nang le phofo ea tšepe e nang le haeterojene e tlase. E sebelisoa ho AC le DC maemong 'ohle. Kaha sekoahelo se na le phofo ea tšepe, se na le ho tjheseletsa ho sebetsang hantle haholo 'me se ka fokotsa likarolo tsa ho tjheseletsa.

Kopo: E sebelisoa bakeng sa ho tjheseletsa tšepe ea carbon le tšepe e tlase ea alloy ea sehlopha sa matla a tsamaellanang, joalo ka Q345, jj.

 

Sebopeho sa lik'hemik'hale sa tšepe e welded (%):

C

Mn

Si

S

P

≤0.12

≤1.60

≤0.75

≤0.030

≤0.035

 

Litšobotsi tsa mechini tsa tšepe e welded:

Ntho ea teko

Matla a tšepe

Mpa

Matla a tlhahiso

Mpa

Ho lelefatsa

%

Boleng ba tšusumetso (J)

(-30℃)

E tiiselitsoe

≥490

≥400

≥22

≥27

E lekiloe

520 ~ 580

≥410

24 ~ 30

50 ~ 180

 

Tekanyo ea haedrojene e hasaneng ea tšepe e bolokiloeng: ≤8.0mL/100g (mokhoa oa glycerin)

Tlhahlobo ea X-ray: Kereiti ea I

 

Khoeli e khothaletsoang:

Bophara ba molamu

(mm)

2.5

3.2

4.0

5.0

5.8

Hona joale ho tjheseletsa

(A)

90 ~ 120

120 ~ 150

170 ~ 200

210 ~ 250

240 ~ 310

 

Tsebiso:

1. Electrode e lokela ho besoa hora e le 'ngoe mochesong oa 350℃ pele ho ts'ebetso ea ho tjheseletsa;

2. Ho bohlokoa ho hlwekisa mafome, sekala sa oli, metsi le litšila likarolong tsa ho tjheseletsa pele ho tjheseletsa;

3. Sebelisa ts'ebetso e kgutshwane ya arc ha o tjheseletsa. Tsela e moqotetsane ya ho tjheseletsa e loketse.

4. Hokela electrode ho palo e ntle ha o sebetsa ho DC.

 

Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka selemo sa 2000. Re 'nile ra kopanela tlhahisong ea li-electrode tsa ho tjheseletsa, lithupa tsa ho tjheseletsa le lisebelisoa tse sebelisoang tsa ho tjheseletsa ka lilemo tse fetang 20.

Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa li-electrode tsa tšepe e sa hloekang, li-electrode tsa tšepe ea khabone, li-electrode tsa ho tjheseletsa tse nang le alloy e tlase, li-electrode tsa ho tjheseletsa tse holim'a metsi, li-electrode tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tse nang le alloy e bobebe le e nang le alloy e tlase, lithapo tsa ho tjheseletsa tse nang le alloy e sirelelitsoeng ke khase, lithapo tsa ho tjheseletsa tsa aluminium, ho tjheseletsa ka har'a arc e ka tlas'a metsi. lithapo, lithapo tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tsa koporo, lithapo tsa ho tjheseletsa tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tse sehang khabone, le lisebelisoa tse ling tsa ho tjheseletsa le tse sebelisoang.

 


  • E fetileng:
  • E 'ngoe: