Terata e nang le motlakase oa E310T1-1/4 FLUX
TLHOPHISO
Sehlopha sa AWS 5.22 E310T1-1/4 / ASME SFA A5.22 Sehlopha sa E310T1-1/4
UNS W31031 A#9 F#6
TLHALOSO
E310T1-1/4 ke terata e sirelelitsoeng ka khase e nang le mothapo o potolohang o etselitsoeng ho tjheseletsa "boemo bohle" 'me e ka sebelisoa le khase e sirelelitsoeng ea 75%Ar / 25%CO2 kapa 100% CO2.
Litekanyetso tsa ho tjheseletsa di lokela ho ntlafatswa ho qoba ho petsoha ho chesang.
LITLHAKISO
E310T1-1/4 e atisa ho sebediswa bakeng sa ho tjheseletsa ditshipi tsa motheo tsa metswako e tshwanang jwalo ka ditshipi tsa AISI 310.
E310T1-1/4 e ka sebediswa bakeng sa ho tjheseletsa tshepe ya khabone ho tshepe e sa ruseng.
E310T1-1/4 e ka sebelisoa bakeng sa ho tjheseletsa kapa ho lokisa lihlooho tse nang le motsoako o phahameng le li-castings tse sa senyeheng tsa motsoako o tšoanang ka kakaretso.
Sebelisa mocheso o tlase o kenang – Fana ka tlhahiso ea 30,000 Joules/In Maximum.
Qoba lifaha tse kobehileng tse tjheseletsang
Boloka mocheso oa interpass o le ka tlase ho 250°F
Tlatsa li-crater tsohle tsa ho qala le ho emisa ho qoba mapetso a li-crater.
KHEMISI E TLWAELEHILENG (%)
| C | Cr | Ni | Mo | Mn | Si | P | S | Cu |
| .10 | 25.9 | 20.4 | .10 | 1.4 | .82 | .015 | .005 | .08 |
LITHEPA TSE TLWAELEHILENG TSA MEKHANIKI
| MATLA A TŠEPE | 89,000 PSI |
| HO ELELLOA KA 2” | 38% |
| Kalafo ea mocheso | HA HO LE E 'NGOE |
Ela Hloko: Thepa ea mechini e bontšitsoeng e sebelisa 100% CO2
LIPARAMETERE TSE TLWAELEHILENG TSA HO WELDA (ho sebelisoa 100% CO2)
| .045” DIA. | E FATILENG & E FETILENG | FOLETE FEELA |
| AMPS | 130-190 | 120-250 |
| LI-VOLT | 24-29 | 25-29 |
| WFS (IPM) | 225-450 | 200-600 |
TLHOKOMELISO: Hlakola 3/8”-1/2”
Fokotsa li-volts ka 2 ha o sebelisa 75%Ar / 25%CO2
Wenzhou Tianyu Electronic Co., Ltd. e thehiloe ka selemo sa 2000. Re ntse re etsa li-electrode tsa ho tjheseletsa,lithupa tsa ho tjheseletsa, le lintho tse sebelisoang ho tjheseletsa ka lilemo tse fetang 20.
Lihlahisoa tsa rona tse ka sehloohong li kenyelletsa li-electrode tsa tšepe e sa hloekang, li-electrode tsa tšepe ea khabone, li-electrode tsa ho tjheseletsa tse nang le alloy e tlase, li-electrode tsa ho tjheseletsa tse holim'a metsi, li-electrode tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tse nang le alloy e bobebe le e nang le alloy e tlase, lithapo tsa ho tjheseletsa tse nang le alloy e sirelelitsoeng ke khase, lithapo tsa ho tjheseletsa tsa aluminium, ho tjheseletsa ka har'a arc e ka tlas'a metsi. lithapo, lithapo tsa ho tjheseletsa tse nang le alloy ea nickel & cobalt, lithapo tsa ho tjheseletsa tsa koporo, lithapo tsa ho tjheseletsa tsa TIG & MIG, li-electrode tsa tungsten, li-electrode tse sehang khabone, le lisebelisoa tse ling tsa ho tjheseletsa le tse sebelisoang.